Multibase Multi-Pro® 3018 XUG Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Multibase
Trade Name Multi-Pro®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Multibase Multi-Pro® 3018 XUG Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Mineral Filled, 30% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureInformation provided by Multibase
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955
Melt Flow 18 g/10 min
18 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.4 MPa
3400 psi
ASTM D638
Elongation at Break 110 %
110 %
ASTM D638
Flexural Modulus 1.93 GPa
280 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
73°F; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 96.1 °C
205 °F
Unannealed; ASTM D648
Processing Properties Metric English Comments
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
Middle Barrel Temperature 193 - 232 °C
380 - 450 °F
Front Barrel Temperature 199 - 232 °C
390 - 450 °F
Nozzle Temperature 193 - 227 °C
380 - 440 °F
Mold Temperature 4.44 - 65.6 °C
40.0 - 150 °F
Drying Temperature 93.3 °C
200 °F
Dry Time 2 hour
2 hour
Back Pressure 0.138 - 0.345 MPa
20.0 - 50.0 psi
Screw Speed 40 - 100 rpm
40 - 100 rpm
Descriptive Properties Value Comments
Clamp Tonnage 2-4 tons/in<sup>2</sup>
Screw L/D Ratio 20:1