Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 199 - 232 °C | 390 - 450 °F | |
Multibase Multi-Pro® 2510 XGW Polypropylene Mineral Filled, 27% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Front Barrel Temperature | 199 - 232 °C | 390 - 450 °F | |
Multibase Multi-Pro® 2516 CU Polypropylene Calcium Carbonate Filler, 25% by weight.Features:Gloss, High UV Resistance, Good Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn and Garden EquipmentInformation provided by Mult.. |
|||
Front Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
RheTech Products FRP102-01 Polypropylene, Flame Retardant, Black Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT1001-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Facias, claddings, and rocker panelsBodyside moldingsStep pads and bumper componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT1002-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT1055-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT1055-685UV Thermoplastic Polyolefin, UV Stabilized, Graphite Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT2500-594UV Thermoplastic Polyolefin, UV Stabilized, 9428NM Spectra Grey Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT2600-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Interior trimSplash shieldsStep pads and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT2700-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Air deflectorsFuel filler shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT3080-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT3080-425 Thermoplastic Polyolefin, UV Stabilized, YBWA Platinum Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT3080-47UV Thermoplastic Polyolefin, UV Stabilized, AYNA Light Prairie Tan Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT3080-50 Thermoplastic Polyolefin, UV Stabilized, YGYA Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT3080-81 Thermoplastic Polyolefin, UV Stabilized, ACRA Titanium Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT4600-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Scuff platesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products P250-247 Polypropylene Copolymer, UV Stabilized, Black Applications: Center consolesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products P252-01 Polypropylene Copolymer, Black Applications: Cowl screenInterior trimBumper coverGlove box binInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products P252-670UV Polypropylene Copolymer, UV Stabilized, 134B Stone Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products P256-670UV Polypropylene Copolymer, UV Stabilized, 134B Stone Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products P256-674UV Polypropylene Copolymer, UV Stabilized, 447B Fawn Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products P257-01 Polypropylene Copolymer, Black Applications: Splash shield and fender linersElectrical enclosuresUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products P261-01 Polypropylene Copolymer, Medium Impact, Black Applications: Radiator grille inlet supportElectrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
Polymer Resources AH-GP1 Acetal Homopolymer, Low Flow, High Melt Strength, Heat Stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
Polymer Resources AH-GP2-TFE10 Acetal Homopolymer, 10% PTFE Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
Polymer Resources AH-GP3-[color]-H Acetal Homopolymer, High Flow Resin, Heat Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 199 °C | 390 °F | |
ExxonMobil Vyram™ 9103-45 Thermoplastic Elastomer
(discontinued **) A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP512-01 High Stiffness Polypropylene Copolymer, UV Stabilized, Black Applications: Automotive interior applicationsSeat back trimCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP501-01 High Performance Polypropylene Copolymer, Non-UV Stabilized, Black Applications: Battery traysInterior TrimInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP501-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Battery traysInterior TrimInjection molding conditions reported in table.Information provided by RheTech Products. |