Processing Properties Metric English Comments
Drying Temperature 93.3 °C
200 °F
Multibase Multi-Pro® 1505 R Polypropylene
Glass Fiber Reinforced, 15% by weight.Features:Heat Resistance, HighScratch ResistantStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Drying Temperature 93.3 °C
200 °F
Multibase Multi-Pro® 1508 M Polypropylene
Mica Filled, 15% by weight.Features:Rigidity, HighImpact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided by Multibase
Drying Temperature 93.3 °C
200 °F
Multibase Multi-Pro® 2514 XU Polypropylene
Mineral Filled, 25% by weight.Features:Heat Resistance, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureTable ProductsInformation provided by Multibase
Drying Temperature 93.3 °C
200 °F
Multibase Multi-Pro® 2518 CU Polypropylene
Calcium Carbonate Filler, 25% by weight.Features:Gloss, High Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Drying Temperature 93.3 °C
200 °F
Multibase Multi-Pro® 3011 CHI Polypropylene
Calcium Carbonate Filler, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Drying Temperature 93.3 °C
200 °F
Multibase Multi-Pro® 3014 XUGW Polypropylene
Mineral Filled.Features:Gloss, HighUV Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn and Garden EquipmentInformation provided by Multibase
Drying Temperature 93.3 °C
200 °F
Multibase Multi-Pro® 4008 T Polypropylene
Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: ConnectorsElectrical/Electronic ApplicationsAppliancesInformation provided by Multibase
Drying Temperature 93.3 °C
200 °F
Multibase Multi-Pro® 4015 THW Polypropylene
Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Lawn and Garden EquipmentTable ProductsFurnitureInformation provided by Multibase
Drying Temperature 93.3 °C
200 °F
Multibase Multi-Pro® 4518 CUW Polypropylene
Calcium Carbonate Filler, 45% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Drying Temperature 93.3 °C
200 °F
Multibase Multi-Pro® 5014 CUW Polypropylene
Calcium Carbonate Filler. Forms:PelletsProcessing Methods:Injection MoldingUses:FurnitureInformation provided by Multibase
Drying Temperature 93.3 °C
200 °F
Oxford Polymers C-Acetal -30GF-Natural Acetal Copolymer, 30% Glass Fiber Reinforced
Product Description: Glass Fiber (30% Reinforced), Co-polymer Acetal, Injection Molding Grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Glass FiberSpecial Characteristic..
Drying Temperature 93.3 °C
200 °F
PolyOne Edgetek® PS-40GF/000 Polybutylene Terephthalate (PBT), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Drying Temperature 93.3 - 121 °C
200 - 250 °F
Average value: 104 °C Grade Count:7
Overview of materials for Polyphenylene Ether, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, PTFE Filled". Each property range of values reported is minimum and maximum values ..
Drying Temperature 93.3 °C
200 °F
then reduce to 160°F
Ecomass® 4703ZG92 Filled Polyurethane
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsModerate Specific GravityFilled Polyurethane (TPU)FlexibleInformation provided by Technical Polymers
Drying Temperature 93.3 - 104 °C
200 - 220 °F
PolyOne Lubri-Tech™ NI-10CF/15T Nylon 6/10, Carbon Fiber Reinforced, PTFE Lubricated  (discontinued **)
Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Drying Temperature 93.3 - 107 °C
200 - 225 °F
Polymer Resources PPX/NY G10 Modified PPO, 10% Glass Reinforced PPX/Nylon 6,6 Alloy  (Unverified Data**)&l
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Drying Temperature 93.3 - 107 °C
200 - 225 °F
Polymer Resources PPX/NY GP1 Modified PPO, General Purpose PPX/Nylon 6,6 Alloy  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.