Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL FE1740PW PPE+PS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL FE1740PW PPE+PS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Noryl* FE1740PW Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; this grade has been developed for fluid engineering applications where higher static stiffness is required. Noryl* FE1740PW has been certified for potable water applications up to 85C in Europe and North America in limited colours.
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Density 1.40 g/cc
0.0506 lb/in³
ISO 1183
Moisture Absorption 0.0600 %
0.0600 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.20 %
0.20 %
ISO 62
Linear Mold Shrinkage, Flow 0.00090 - 0.0015 cm/cm

@Thickness 3.20 mm
0.00090 - 0.0015 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 10 g/10 min

@Load 5.00 kg,
Temperature 300 °C
10 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
Melt Index of Compound 20 g/10 min

@Load 10.0 kg,
Temperature 300 °C
20 g/10 min

@Load 22.0 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 155 MPa
22500 psi
5 mm/min; ISO 527
165 MPa
23900 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 1.8 %
1.8 %
Type I, 5 mm/min; ASTM D638
1.8 %
1.8 %
5 mm/min; ISO 527
Tensile Modulus 11.3 GPa
1640 ksi
1 mm/min; ISO 527
13.8 GPa
2000 ksi
5 mm/min; ASTM D638
Flexural Strength 195 MPa
28300 psi
2 mm/min; ISO 178
225 MPa
32600 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 9.50 GPa
1380 ksi
2 mm/min; ISO 178
11.7 GPa
1700 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
0.900 J/cm

@Temperature -30.0 °C
1.69 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
80*10*4; ISO 180/1U
30.0 kJ/m²

@Temperature -30.0 °C
14.3 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched 3.00 J/cm²
14.3 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Dart Drop, Total Energy 18.0 J

@Temperature 23.0 °C
13.3 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
11.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 147 °C
297 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
148 °C

@Thickness 3.20 mm
298 °F

@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 151 °C
304 °F
Rate B/50; ASTM D1525
152 °C
306 °F
Rate B/50; ISO 306
161 °C
322 °F
Rate B/120; ISO 306