Material Notes:
Medium-hard silicone binder resin for maintenance paints, colored baking enamels, decorative finishes. Improves heat resistance and weathering of organic resins. As an additive to improve flow-out of epoxy paints and initial gloss.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc

@Temperature 25.0 °C
1.06 g/cc

@Temperature 77.0 °F
Viscosity 10 - 30 cP
10 - 30 cP
dynamic
Thermal Properties Metric English Comments
Flash Point 7.00 °C
44.6 °F
closed cup
Processing Properties Metric English Comments
Shelf Life 21.0 Month
21.0 Month
Descriptive Properties Value Comments
Color pale straw
Resin Content (%) 60
Water Resistant yes