Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | ASTM D955-95 |
Multibase Multi-Flex® TPO 1047-3000 The burn rate is 0.53 in/min; ASTM FM VSS 302.Data provided by Multibase. |
|||
Linear Mold Shrinkage | 0.010 - 0.030 cm/cm | 0.010 - 0.030 in/in | |
Multibase TPSiV® 4200-70A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e.. |
|||
Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | |
Nylene® 6111 (HS) , 40% Glass/Mineral Reinforced Nylon 6/6 Description: Nylene® 6111 (HS) is a 40% mineral reinforced, impact modified nylon 6/6. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Pol.. |
|||
Linear Mold Shrinkage | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPC T3020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.019 cm/cm | 0.010 - 0.019 in/in | FRISETTA Test Method |
Nilit FRIANYL B63 KV15 Nylon 6 for injection molding, 15% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | ASTM D955-89 |
Multibase Multi-Pro® 3019 CXUW High Gloss 30% TiO2 Filler Content Polypropylene Multi-Pro 3019 CXUW is a mineral reinforced polypropylene compound exhibiting high stiffness and impact characteristics. This material was specially formulated with UV stabilization for outdoor app.. |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PP EVR8025H UV Polypropylene/EDPM, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPC T2020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.018 cm/cm @Thickness 3.17 mm |
0.010 - 0.018 in/in @Thickness 0.125 in |
ASTM D 955 |
RTP Company RTP 800 MG 20 TFE 15 Acetal (POM), Milled Glass - PTFE Lubricated |
|||
Linear Mold Shrinkage | 0.010 - 0.013 cm/cm | 0.010 - 0.013 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYform POM C M90 GF30 Polyoxymethylene Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 - 0.020 cm/cm @Thickness 3.17 mm |
0.010 - 0.020 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company RTP PA66 L BLK Nylon 6/6 (PA), Value Product - Lubricated - Heat Stabilized |
|||
Linear Mold Shrinkage | 0.010 - 0.016 cm/cm | 0.010 - 0.016 in/in | |
Lehmann & Voss LUVOCOM® 1105-7197/BK PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts.Improved friction and wear behaviour. Emergency r.. |
|||
Linear Mold Shrinkage | 0.010 - 0.016 cm/cm | 0.010 - 0.016 in/in | |
Lehmann & Voss LUVOCOM® 1105-7198/BK PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Linear Mold Shrinkage | 0.010 - 0.016 cm/cm | 0.010 - 0.016 in/in | |
Lehmann & Voss LUVOCOM® 1105-8264 PEEK, with CNT Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Electrically conductive, suitable for continuous discharging of statically generated elect.. |
|||
Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | ASTM D995 |
Huntsman IROGRAN® A 92 K 5031 TPU-High Temperature Performance Polycaprolactone and ether based. Good processability and compression set. Excellent resistance to high temperatures, water, grease, and oils.. Used in seals, wheels, and rollers.Information prov.. |
|||
Linear Mold Shrinkage | 0.010 cm/cm @Temperature 150 °C, Time 900 sec |
0.010 in/in @Temperature 302 °F, Time 0.250 hour |
DIN 40634 |
Mitsubishi Hostaphan® RN, 100 micron Nominal Thickness Universal Polyethylene Terephthalate Film Hostaphan® RN is a biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties.Applications:Films for industrial applicationsCoatingLamin.. |
|||
Linear Mold Shrinkage | 0.010 - 0.016 cm/cm | 0.010 - 0.016 in/in | |
Lehmann & Voss LUVOCOM® 1105-7285/EM/BL PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | ASTM D955 |
Multibase Multi-Flex® 1047-0000 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsI.. |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | ASTM D955 |
Teknor Apex APEX® 4103 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | ASTM D955 |
Teknor Apex APEX® 4111 Polyvinyl Chloride, Flexible Notes: 105°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain Reliefs; Wire and Cable ApplicationsForms: Pellets Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molded Comp.. |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | ASTM D955 |
Teknor Apex APEX® 6500-90 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Linear Mold Shrinkage | 0.010 - 0.014 cm/cm @Thickness 3.20 mm |
0.010 - 0.014 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 301 Ionomer Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.010 - 0.020 cm/cm @Thickness 3.20 mm |
0.010 - 0.020 in/in @Thickness 0.126 in |
ASTM D 955 |
RTP Company RTP 200 AR 10 TFE 10 SI 2 Nylon 6/6 (PA) Aramid Fiber - PTFE Lubricated - Silicone Lubricated |
|||
Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | |
Polyram RamOfin PPH353M8 Polypropylene, 40% Mineral Filled 40% mineral filled polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | ASTM Data MD |
BASF Capron® 8360 HS 34% Mineral-Filled Nylon 6 (Dry)
(discontinued **) Capron 8360 HS is a heat stabilized 34% mineral reinforced nylon 6 injection molding resin possessing a high level of toughness and ductility combined with excellent processability and surface aesth.. |
|||
Linear Mold Shrinkage | 0.010 - 0.012 cm/cm | 0.010 - 0.012 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPH T8020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.010 cm/cm | 0.010 in/in | ASTM Data; MD |
BASF Ultramid® C33 01 PA66/6 (Dry) Ultramid C33 01 is an intermediate viscosity PA6/66 grade. Its lower melting point than standard PA6 is advantageous for coextrusion with temperature sensitive polymers like EVOH. It conforms to F.. |
|||
Linear Mold Shrinkage | 0.010 - 0.025 cm/cm | 0.010 - 0.025 in/in | ASTM D955 |
BP Amoco Amoco® 7635 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: High stiffness, Nucleated, AntistaticTypical applications: Rigid packaging, Consumer productsComplies with FDA specification, Title 21, CFR .. |
|||
Linear Mold Shrinkage | 0.010 - 0.025 cm/cm | 0.010 - 0.025 in/in | ASTM D955 |
BP Amoco Amoco® Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection molding; Rotary CompressionFeatures: Nucleated, Antistatic, LubricatedTypical applications: Closures, CapsComplies with FDA specification, Title 21, CFR 177... |
|||
Linear Mold Shrinkage | 0.010 - 0.025 cm/cm | 0.010 - 0.025 in/in | ASTM D955 |
BP Amoco Acctuf® 3638 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Compounding, AntistaticComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded samples. |