Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM D648 |
Multibase Multi-Pro® 3018 XUG Polypropylene Mineral Filled, 30% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureInformation provided by Multibase |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 3.20 mm |
205 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycolac® MG29 ABS Super high impact ABS. Good low temperature toughness. High gloss. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM D648 |
Multibase Multi-Pro® 2510 XG Polypropylene Mineral Filled, 25% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureInformation provided by Multibase |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | Annealed; ISO 75-2A |
Total Lacqrene® 1070 Crystal Polystyrene
(discontinued **) Description: LACQRENE® 1070 is a very high molecular weight polystyrene used in extrusion. It is particularly designed for the production of foam sheet, where the very high molecular weight gives .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | |
Polimeri Europa SINKRAL B633/E ABS, Impact & Heat Stabilized Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,EG,105-04-25-20 High impact extrusion grade with excellent stiffness, good processability and high thermal stabili.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | |
Polimeri Europa SINKRAL C333/m² ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,105-04-16-20 Special low gloss grade for injection moulding which combines medium heat resistance with a good b.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | ASTM D648 |
Flint Hills P4G3A-052 Homopolymer Polypropylene Features: Long Term Heat Aging (LTHA). Product does not contain animal derived components. Phthalate-free.Applications: Injection MoldingInformation provided by Flint Hills Resources. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | ISO 75-1,-2 |
Ineos ABS Triax® KU2-3154 ABS + Polyamide Blend (Conditioned), Injection Molding Grade Triax® KU2-3154 is mineral reinforced, easy-flowing, injection molding grade, and comes in pellets. It has reduced moisture absorption and very low warpage. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 6.35 mm |
205 °F @Thickness 0.250 in |
ASTM D648 |
IRPC Polimaxx Porene GA800 Acrylonitrile Butadiene Styrene Applications:injection moldinghousing of electrical appliances such as electric fans, telephones, calculators and toys |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 6.35 mm |
205 °F @Thickness 0.250 in |
ASTM D648 |
IRPC Polimaxx Porene GA850 Acrylonitrile Butadiene Styrene Applications:injection moldinghousing of electrical appliances such as electric fans, telephones, calculators and toys |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | |
Ineos ABS TRIAX® 1220 S ABS/Nylon Blend, As Conditioned Extrusion and injection molding grade with good stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical dampi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 3.20 mm |
205 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Xylex X7200MR PC+POLYESTER (Asia Pacific) Mold Release version of X7200This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 3.20 mm |
205 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS (Asia Pacific) LNP* Stat-loy* AF3009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Antistat, Flame Retardant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Thermocomp MX05038 PP (Europe-Africa-Middle East) Polypropylene compound, containing miniral. Added features include High ImpactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM Data |
Styron Magnum™ 344CC ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® HIPS FR-1 Availability: North AmericaForms: PelletsFeatures: Flame RetardantRoHS Compliance: RoHS CompliantInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 3.17 mm |
205 °F @Thickness 0.125 in |
unannealed; ASTM D648 |
Stratasys® ABS-M30 ABS-M30 is 25-70 percent stronger than standard Stratasys ABS and is an ideal material for conceptual prototyping, design verification, and direct digital manufacturing. ABS-M30 has greater tensile,.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | ISO 75-2 |
Borealis BH374MO Polypropylene Copolymer BH374MO is a heterophasic copolymer. This grade is characterized by optimum combination of very high stiffness, good flow properties and good impact strength. Products molded with this grade exhibi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | ISO 75-2 |
Borealis Daplen™ HJ060UB Polypropylene Compound for Direct Left Manufactured Applications Daplen FJ060UB is a special low viscosity compound for direct LFT manufacturing process. It interacts perfectly with glass fibers to create excellent stiffness and impact resistance. Daplen HJ060U.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | 0.250 inch; ASTM D648 |
TPI Porene® GA800TW High Gloss/Weather Resistant/Antistatic Grade ABS INJECTION MOLDING; ANTISTATIC; WEATHER RESISTANT. HOUSING OF ELECTRICAL APPLIANCES, e.g. ELECTRIC FAN, TELEPHONE, CALCULATOR, TOYSPorene® is a registered trademark of Thai Petrochemical Industry C.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | Annealed; ISO 75-2A |
Total PSC 1960N Crystal Polystyrene 1960N is a high resistance crystal polystyrene with very high flow for the production of thick insulation board. The very low viscosity of this grade makes it particularly suitable for the producti.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | ASTM D648 |
TPI Porene® ABS-GA800 High Impact ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | ASTM D648 |
Engineered Polymer Solutions ABS 550 Medium Impact. Natural and colors available. Medium gloss. Injection molding grade. Uses: General PurposeInformation provided by Engineered Polymer Solutions. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | ASTM D648 |
Aclo Accutech ABS ABS832G10L Glass Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | ASTM D-648 |
Axiall HHP-190 Rigid PVC, Extrusion Georgia Gulf HHP-190 is a special purpose profile extrusion alloy designed for applications requiring the following properties: Heat Resistance & Thermal StabilityImpact Strength & ToughnessDimensi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | 5% Cloisite® reinforced Nylon 6 |
BYK Cloisite® 20A Nanoclay Cloisite® 20A is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.Information provided by Southern Clay ProductsSouthern Clay Pr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | ISO 75-2 |
CENTROPLAST CENTRODAL C FG Polyoxymethylene, Food Grade POM C is a partially crystalline thermoplastic, which is characterized by its excellent machinability, dimensional stability, and chemical resistance.Information provided by CENTROPLAST Engineering .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 - 205 °C | 205 - 401 °F | Average value: 149 °C Grade Count:153 |
Overview of materials for Polypropylene with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C | 205 °F | 5% Cloisite® reinforced Nylon 6 |
BYK Cloisite® 30B Nanoclay Cloisite® 30B is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.
Information provided by Southern Clay ProductsSouthern Clay P.. |