Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 23.4 MPa | 3400 psi | ASTM D638 |
Multibase Multi-Pro® 3014 XUGW Polypropylene Mineral Filled.Features:Gloss, HighUV Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn and Garden EquipmentInformation provided by Multibase |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | ASTM D638 |
Multibase Multi-Pro® 3018 XUG Polypropylene Mineral Filled, 30% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureInformation provided by Multibase |
|||
Tensile Strength, Yield | 23.4 MPa | 3390 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable W3204 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | >= 23.4 MPa | >= 3400 psi | ASTM D638 |
S&E Specialty Polymers TufGuard M™ GPP1005M-EXLT PP, Flame Retardant Application: UL94 V-2, Non-blooming flame retardant polypropylene compound for injection molding.Information provided by S&E Specialty Polymers |
|||
Tensile Strength, Yield | 23.4 MPa | 3390 psi | press cure 11 min./160ºC |
TSE Industries Millathane® 26 Millable Polyether Urethane for Food Contact Applications Millathane 26 is a polyether polyurethane rubber compliant with the United States Code of Federal Regulations*, Title 21 parts 177.1680 and 177.2600. This polyurethane rubber is designed for food co.. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | aged 70 hours at 250ºF in ASTM Oil #903 |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical) MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 23.4 MPa | 3390 psi | ASTM D638 |
Chevron Phillips LX8119 HDPE Injection Molding Resin
(discontinued **) Resin Type: linear copolymer; ASTM D4976 Classification: PE 233, A 56700Characteristics: warp resistant, excellent impact strength, excellent ESCR, moderate shrinkage resistanceApplications: seats, .. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | ASTM D638 |
LyondellBasell Petrothene® LP5002 High Density Polyethylene (Blow Molding Grade) ApplicationsThe PETROTHENE LP series of polyethylene resins exhibits excellent environmental stress crack resistance and is especially designed for bottles containing aggressive agricultural and hou.. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | ASTM D638 |
Fiberfil® PP-61/TC/20 Polypropylene Copolymer, 20% Talc Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | 2"/min; ASTM D638 |
Garland Manufacturing GAR-DUR® Ultra High Molecular Weight Polyethylene (UHMW-PE) GAR-DUR® plastic parts are made from ultra high molecular weight (UHMW) polymer having a molecular weight of 4.2 million and greater. Garland Manufacturing Company has been processing UHMW resin .. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | ASTM D638 |
Global CPP-140 40% CaC03 Filled, Polypropylene Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 23.4 MPa | 3390 psi | 2 in/min.; ASTM D638 |
Ineos K46-06-185 HDPE K46-06-185 is a natural high molecular weight, high-density copolymer polyethylene developed for automotive fuel tanks. It combines excellent processability and outstanding physical performance, par.. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | ASTM D638 |
Ineos L70Z-01 Polypropylene Impact Copolymer L70Z-01 is a nucleated and antistatic high flow polypropylene medium impact copolymer for injection molding applications. This product meets the requirements of the U.S. Food and Drug Administration.. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | ASTM D638 |
Techmer ES HiFill® HIPS 484 GY Availability: North AmericaForms: PelletsAppearance: GreyInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | ASTM D638 |
Techmer ES HiFill® HIPS LE BK Availability: North AmericaForms: PelletsAppearance: BlackTPCI# 8813148Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | ASTM D 638 |
Styrolution Zylar 960 MBS ZYLAR 960 is an impact modified styrene acrylic copolymer that provides toughness equivalent to some grades of polycarbonate, good clarity and superior processing characteristics for demanding injec.. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | ASTM D638 |
A. Schulman LP481 Molding Grade High-Density Polyethylene DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | aged 70 hours at 250ºF in ASTM Oil #903 |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical) MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | (2.0 in/min); ASTM D638 |
ExxonMobil HDPE HD P8760.29 High Density Polyethylene Resin Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum bal.. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | Molded and tested in accordance with ASTM D4976; ASTM D638 |
Dow DOWLEX™ IP-51 High Density Polyethylene Resin (HDPE) DOWLEX™ IP-51 is an Improved Processing high density resin designed to offer excellent process-ability and impact performance. This resin was designed by optimization of the breadth, shape and pea.. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | Molded and tested in accordance with ASTM D4976; ASTM D638 |
Dow UNIVAL™ DMDC-6143 NT 7 High Density Polyethylene Resin (HDPE) Excellent parison melt strength / low sag Good extrudability / process-ability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDC-6143 NT 7 is a polymer with broad molecular weight distri.. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | ASTM D638 |
ExxonMobil HD 6605.70 Injection Molding Resin Product Description: HD 6605.70 is a narrow molecular weight hexane copolymer designed for a wide range of injection molding applications, offering excellent ESCR with good stiffness-toughness balan.. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | ASTM D638 |
Entec Hyrene® PS-HI 3/2 High Impact Polystyrene Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | 50 mm/min; ASTM D638 |
Amco PRIMATOP PP CO 350-20 Impact Polypropylene Copolymer PP CO 350-20 has easy mold flow and excellent dimensional stability. It is used in thin walled injection molded applications.Former A-Top Polymers product; part of Amco product line since 2013. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | after 7 days at 100ºC |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 1.5 PHR Sulfur MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | ASTM D638 |
Amco Amalloy® B1017 Polymer Alloy Amco Amalloy B1017 is a clear performance copolymer with exceptional clarity and toughness.High melt-flow, very clear.Information provided by Amco Plastic Materials. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | 2.0 in/min; ASTM D638 |
ExxonMobil HD 8760.29 Rotational Molding Resin Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum bal.. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | at 100%; ASTM D412 |
EG72D Polyurethane-based Biomedical Elastomer |