Processing Properties Metric English Comments
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
Multibase Multi-Pro® 2510 XGW Polypropylene
Mineral Filled, 27% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
Multibase Multi-Pro® 3014 XUGW Polypropylene
Mineral Filled.Features:Gloss, HighUV Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn and Garden EquipmentInformation provided by Multibase
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products FT4900-01UV Thermoplastic Polyolefin, UV Stabilized, Black
Applications: Exterior componentsBodyside moldingsStep padsLicense plate bracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products FT4900-33UV Thermoplastic Polyolefin, UV Stabilized, KSD Charcoal Argent
Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products FT4900-659UV Thermoplastic Polyolefin, UV Stabilized, ZSP Deep Grey
Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products FT4900-772UV Thermoplastic Polyolefin, UV Stabilized, RXF Jet Black
Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products G10P100-01UV 10% Glass Fiber Reinforced Polypropylene, UV Stabilized, Black
Applications: BracketsIP structural componentsDome light housingInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products G10UP100-01 10% Glass Fiber Reinforced Polypropylene, Black, UL94-HB Rated
Applications: Consumer housingsConsumer goodsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products G13P100-332UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (GM 9772) Light Neutral
Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products G13P100-553UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (GM 501F) Dark Smoke Gray
Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products GC10P100-01 10% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black
Applications: Air ducts - distributionFuel filler pocketsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products GC10P200-01 10% Glass Fiber Reinforced Polypropylene Copolymer, Non-UV Stabilized, Chemically Coupled, Black
Applications: HousingsStorage binsBracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products HP514-182 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 7701 Graphite
Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products HP514-489 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 101E Lite Oak
Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products HP521-01 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black
Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products HP521-186 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 7701 Graphite
Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products HP521-188 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 9777 Medium Beige
Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products HP521-231 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 173B Navy Blue
Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products T10P250-00 10% Talc Reinforced Polypropylene Copolymer, Natural
Applications: Fan shroudsCenter consolesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products T10UP100-01 10% Talc Reinforced Polypropylene Copolymer, General Purpose Black, UL94 HB Rated
Applications: Wire troughElectrical componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 204 °C
380 - 400 °F
Polymer Resources AH-GP2 Acetal Homopolymer, Medium Flow, Heat Stabilized
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Rear Barrel Temperature 193 °C
380 °F
ExxonMobil Santoprene® 243-40 Thermoplastic Elastomer  (discontinued **)
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f..
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products HP522-473 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, ZU5A Dark Graphite
Applications: ConsolesClose out panelInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 °C
380 °F
PTS Trilac® ABS-HS6500 High Impact ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 193 °C
380 °F
ExxonMobil Santoprene® 123-40 Thermoplastic Elastomer
A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran..
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
Multibase Multi-Pro® 4007 XGS Polypropylene
Mineral, 40% by weight.Features:Gloss, HighScratch ResistantForms:PelletsProcessing Methods:Injection MoldingUses: FurnitureAppliancesInformation provided by Multibase
Rear Barrel Temperature 193 - 204 °C
380 - 400 °F
Polymer Resources AH-GP1 Acetal Homopolymer, Low Flow, High Melt Strength  (Unverified Data**)
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Rear Barrel Temperature 193 - 204 °C
380 - 400 °F
Kraton® G7720 GI-N (SEBS) Compound
Description: Kraton G7720 GI-N is an easy processing, general purpose 57 Shore a hardness material designed for a wide variety of applications. It is supplied from North America in the physical form..
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products GC15P200-01 15% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Electrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products HP508-01UV 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black
Applications: Interior trim, Close out panelsConsolesInjection molding conditions reported in table.Information provided by RheTech Products.