Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol ESTANE® 54640 Ether Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 54640 Ether Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Very good physical properties and hydrolysis resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusionAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Maximum Moisture Content 0.020
0.020
Mechanical Properties Metric English Comments
Hardness, Shore A 82 - 88
82 - 88
ASTM D2240
Tensile Strength 45.5 MPa
6600 psi
ASTM D412
Elongation at Break 650 %
650 %
ASTM D412/D638
100% Modulus 0.00620 GPa
0.899 ksi
ASTM D412
300% Modulus 0.0117 GPa
1.70 ksi
ASTM D412
Tear Strength 21.0 kN/m
120 pli
Trouser; ASTM D470
Graves Tear Strength 68.4 kN/m
390 pli
Die C; ASTM D624
Tensile Set 14 %
14 %
200% elongation; ASTM D412
Thermal Properties Metric English Comments
Melting Point 135 °C
275 °F
DSC
Glass Transition Temp, Tg -49.0 °C
-56.2 °F
DSC
Processing Properties Metric English Comments
Zone 1 171 °C
340 °F
Extrusion
Zone 2 177 °C
351 °F
Extrusion
Zone 3 182 °C
360 °F
Extrusion
Zone 4 188 °C
370 °F
Extrusion
Adapter Temperature 188 °C
370 °F
5, Extrusion
Die Temperature 188 °C
370 °F
Zone 1, Extrusion
188 °C
370 °F
Zone 2, Extrusion
Melt Temperature 185 °C
365 °F
Drying Temperature 104 °C
219 °F
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Dew Point -40.0 °C
-40.0 °F
Descriptive Properties Value Comments
Volume Swell in Water 1.3%
24h/23°C