Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 300% Modulus = 0.0117 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.0117 GPa
1.70 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Sundex 790 Plasticizer
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.0117 GPa
1.70 ksi
Injection molded parts; DIN 53504
Huntsman IROGRAN® A 85 E 4719 TPU-Polyester
Introduction: IROGRAN A 85 E 4719 is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offers a..
300% Modulus 0.0117 GPa
1.70 ksi
Injection molded parts; DIN 53504
Huntsman IROGRAN® A 85 E 5719 FCM TPU-Polyester
Introduction: IROGRAN A 85 E 5719 FCM is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offe..
300% Modulus 0.0117 - 0.0152 GPa
1.70 - 2.20 ksi
ASTM D412
Huntsman KRYSTALFLEX® PE 399 Polyurethane Optical Aliphatic Film
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers
300% Modulus 0.0117 GPa
1.70 ksi
ASTM D412
SK Chemicals SKYTHANE® S180A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
300% Modulus 0.0117 GPa
1.70 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Sundex 790 Plasticizer
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.0117 GPa
1.70 ksi
ASTM D412
Lubrizol Estane® 2103-80AE Thermoplastic Polyurethane Elastomer
Formerly PellethaneAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
300% Modulus 0.0117 GPa
1.70 ksi
ASTM D412
Lubrizol Estane® 2103-84AEN Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Contains UV Stabilizer, NSF Standard 61 certifiedAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pelletha..
300% Modulus 0.0117 GPa
1.70 ksi
ASTM D412
Lubrizol ESTANE® 54640 Ether Based Thermoplastic Polyurethane
Very good physical properties and hydrolysis resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusionAvailable in Americas, Europe, Middle E..
300% Modulus 0.0117 - 0.0138 GPa
1.70 - 2.00 ksi
Secant; Conditioned 7 days at RT/50% RH; ASTM D638
AdvanSource Biomaterials ChronoFlex® C 55D Biodurable Medical Grade Polyurethane
ChronoFlex® C is a family of premium polycarbonate aromatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® C medical-grade elastome..
300% Modulus 0.0117 GPa
1.70 ksi
ASTM D412
Lubrizol ESTANE® 58311 Ether Based Thermoplastic Polyurethane
Features: Very good physical properties, hydrolysis resistance, low temperature performance and abrasion. Wide processing window for extrusion.Uses: Flat Die/Cast Film Extrusion, Profile ExtrusionAv..
Copyright © lookpolymers.com All Rights Reserved