Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Die Temperature = 188 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Die Temperature 188 °C
370 °F
Zone 3
Premix Thermoplastics PRE-ELEC® ESD 7100
PRE-ELEC ESD 7100 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7100 has been developed for inject..
Die Temperature 188 °C
370 °F
Zone 5
Premix Thermoplastics PRE-ELEC® ESD 7120
PRE-ELEC ESD 7120 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7120 has been developed for inject..
Die Temperature 188 °C
370 °F
Zone 2
Premix Thermoplastics PRE-ELEC® ESD 7120
PRE-ELEC ESD 7120 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7120 has been developed for inject..
Die Temperature 188 °C
370 °F
Zone 3
Premix Thermoplastics PRE-ELEC® ESD 7120
PRE-ELEC ESD 7120 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7120 has been developed for inject..
Die Temperature 188 °C
370 °F
Zone 4
Premix Thermoplastics PRE-ELEC® ESD 7120
PRE-ELEC ESD 7120 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7120 has been developed for inject..
Die Temperature 188 °C
370 °F
Zone 1
Premix Thermoplastics PRE-ELEC® ESD 7120
PRE-ELEC ESD 7120 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7120 has been developed for inject..
Die Temperature 188 °C
370 °F
Zone 3
Premix Thermoplastics PRE-ELEC® ESD 7200
PRE-ELEC ESD 7200 is a static dissipative thermoplastic compound based on PC/ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7200 has been developed for inj..
Die Temperature 188 °C
370 °F
Zone 4
Premix Thermoplastics PRE-ELEC® ESD 1100  (discontinued **)
PRE-ELEC ESD 1100 is a static dissipative thermoplastic compound based on PETG. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 1100 has been developed for the e..
Die Temperature 188 °C
370 °F
Zone 1
Premix Thermoplastics PRE-ELEC® ESD 1100  (discontinued **)
PRE-ELEC ESD 1100 is a static dissipative thermoplastic compound based on PETG. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 1100 has been developed for the e..
Die Temperature 188 °C
370 °F
Zone 2
Premix Thermoplastics PRE-ELEC® ESD 1100  (discontinued **)
PRE-ELEC ESD 1100 is a static dissipative thermoplastic compound based on PETG. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 1100 has been developed for the e..
Die Temperature 188 °C
370 °F
Zone 5
Premix Thermoplastics PRE-ELEC® ESD 1100  (discontinued **)
PRE-ELEC ESD 1100 is a static dissipative thermoplastic compound based on PETG. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 1100 has been developed for the e..
Die Temperature 188 °C
370 °F
Zone 2, Extrusion
Lubrizol ESTANE® 58244 Ether Based Thermoplastic Polyurethane
Features: Non-Halogenated flame retardant compoundUses: Extrusion – wire and cable and general extrusion where flame retardant propertied are requiredAvailable in Americas, Europe, Middle East, Afr..
Die Temperature 188 °C
370 °F
Zone 2, Extrusion
Lubrizol ESTANE® 58370 Ether Based Thermoplastic Polyurethane
Features: Halogenated flame retardant compoundUses: Extrusion – Wire and cable and general application where flame retardant properties are neededAvailable in Americas, Europe, Middle East, Africa,..
Die Temperature 188 °C
370 °F
Zone 1, 6, Extrusion
Lubrizol ESTANE® 54610 Ester Based Thermoplastic Polyurethane
Features: Good physical properties and chemical resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusion.Available in Americas, Europe, Midd..
Die Temperature 188 °C
370 °F
Zone 2, Extrusion
Lubrizol ESTANE® 54610 Ester Based Thermoplastic Polyurethane
Features: Good physical properties and chemical resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusion.Available in Americas, Europe, Midd..
Die Temperature 188 °C
370 °F
Zone 1, Extrusion
Lubrizol ESTANE® 54640 Ether Based Thermoplastic Polyurethane
Very good physical properties and hydrolysis resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusionAvailable in Americas, Europe, Middle E..
Die Temperature 188 °C
370 °F
Zone 2, Extrusion
Lubrizol ESTANE® 54640 Ether Based Thermoplastic Polyurethane
Very good physical properties and hydrolysis resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusionAvailable in Americas, Europe, Middle E..
Die Temperature 188 °C
370 °F
6, Zone 1, Extrusion
Lubrizol ESTANE® 58315 Ether Based Thermoplastic Polyurethane
Features: Very good physical properties, hydrolysis resistance, low temperature performance and abrasion. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection..
Die Temperature 188 °C
370 °F
Zone 2, Extrusion
Lubrizol ESTANE® 58315 Ether Based Thermoplastic Polyurethane
Features: Very good physical properties, hydrolysis resistance, low temperature performance and abrasion. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection..
Die Temperature 188 °C
370 °F
Zone 1, 6, Extrusion
Lubrizol ESTANE® 58202 Ether Based Thermoplastic Polyurethane
Features: Halogenated flame retardant compound with good low temperature properties and cut resistanceUses: Extrusion – wire and cable jacketing and general extrusion where flame retardant properti..
Die Temperature 188 °C
370 °F
Zone 2, Extrusion
Lubrizol ESTANE® 58202 Ether Based Thermoplastic Polyurethane
Features: Halogenated flame retardant compound with good low temperature properties and cut resistanceUses: Extrusion – wire and cable jacketing and general extrusion where flame retardant properti..
Die Temperature 188 °C
370 °F
Zone 1, Extrusion
Lubrizol ESTANE® 58311 Ether Based Thermoplastic Polyurethane
Features: Very good physical properties, hydrolysis resistance, low temperature performance and abrasion. Wide processing window for extrusion.Uses: Flat Die/Cast Film Extrusion, Profile ExtrusionAv..
Die Temperature 188 °C
370 °F
Zone 2, Extrusion
Lubrizol ESTANE® 58311 Ether Based Thermoplastic Polyurethane
Features: Very good physical properties, hydrolysis resistance, low temperature performance and abrasion. Wide processing window for extrusion.Uses: Flat Die/Cast Film Extrusion, Profile ExtrusionAv..
Copyright © lookpolymers.com All Rights Reserved