Mechanical Properties Metric English Comments
Tensile Strength 45.5 MPa
6600 psi
ASTM D638
PolyOne Novablend™ 6602 Polyvinyl Chloride, Rigid (PVC, Rigid)
Novablend 6602 is a rigid, opaque PVC for molding compounds. This product has high impact, excellent indoor/outdoor weathering, high flow, and good processing characteristics.Applications includes: ..
Tensile Strength 45.5 MPa

@Temperature 75.0 °C,
Time 605000 sec
6600 psi

@Temperature 167 °F,
Time 168 hour
30 mil sheet, Immersion in Water
Lubrizol ESTANE® 58887 Ether Based Thermoplastic Polyurethane
Features: Excellent hydrolysis resistance, low temperature performance, clarity and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and blow molding; cab..
Tensile Strength 45.5 MPa
6600 psi
ASTM D412
Lubrizol ESTANE® 54640 Ether Based Thermoplastic Polyurethane
Very good physical properties and hydrolysis resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusionAvailable in Americas, Europe, Middle E..
Tensile Strength 45.5 MPa
6600 psi
ASTM D638
Ensinger XP-154 Compression Molded PI Compound, 40% Graphite, Premium Grade
The XP 150 Series are amorphous high performance polyimides with high permanent temperature and creep resistance, as well as excellent bearing and wear properties, and excellent long term thermal st..
Tensile Strength 45.5 MPa
6600 psi
Cross; ASTM D882
Arlon CuClad 217 PTFE/Woven Fiberglass Laminate Microwave Printed Circuit Board Substrate
CuClad 217 uses a low fiberglass/PTFE ratio to provide the lowest dielectric constant and dissipation factor available in fiberglass reinforced PTFE based laminates. Together, these properties offe..
Tensile Strength 45.5 - 59.3 MPa
6600 - 8600 psi
Bulk Molding Compounds BMC T60-6002A-WG Wear Resistant Molding Compound
BMC T60-6002A-WG is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost pe..
Tensile Strength 45.5 - 59.3 MPa
6600 - 8600 psi
Bulk Molding Compounds BMC T60-6002-WG(15) Wear Resistant Molding Compound
BMC T60-6002-WG-(15) is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cos..
Tensile Strength 45.5 MPa
6600 psi
ASTM D638
Aaron Industries AAROPRENE® AEN 6600-3 Nylon 6/6 Engineered Resin
Tensile Strength 45.5 MPa
6600 psi
ASTM D412
Lubrizol ESTANE® 58311 Ether Based Thermoplastic Polyurethane
Features: Very good physical properties, hydrolysis resistance, low temperature performance and abrasion. Wide processing window for extrusion.Uses: Flat Die/Cast Film Extrusion, Profile ExtrusionAv..