Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 177 - 204 °C | 351 - 399 °F | |
PolyOne Versalloy™ HC 9220-70 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-70 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
Zone 2 | 177 - 204 °C | 351 - 399 °F | |
PolyOne Versalloy™ HC 9220-80 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-80 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
Zone 2 | 177 - 204 °C | 351 - 399 °F | |
PolyOne Versalloy™ HC 9220-90 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-90 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
Zone 2 | 177 - 193 °C | 350 - 380 °F | |
LyondellBasell Petrothene® GA837091 Medium Density Polyethylene
(Unverified Data**) ApplicationsPETROTHENE GA 837-091 is a broad molecular weight, medium density resin designed for use as a base resin in wire and cable jacketing. An antioxidant has been added to ensure thermal st.. |
|||
Zone 2 | 177 - 204 °C | 350 - 400 °F | |
LyondellBasell Alathon® M5370WC High Density Polyethylene ApplicationsALATHON M 5370WC is a natural, high density, polyethylene copolymer resin with a narrow molecular weight distribution formulated for use as primary insulation for coaxial and control cab.. |
|||
Zone 2 | 177 - 204 °C | 350 - 400 °F | |
LyondellBasell Alathon® M6080WC High Density Polyethylene ApplicationsALATHON M 6080WC is a natural, high density, polyethylene homopolymer resin with a narrow molecular weight distribution formulated for use as primary insulation for coaxial and control c.. |
|||
Zone 2 | 177 - 193 °C | 350 - 380 °F | |
LyondellBasell Petrothene® GA808091 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 808-091 is a broad molecular weight, linear low density polyethylene resin designed for use as a base resin in wire and cable jacketing. An antioxidant package is added to.. |
|||
Zone 2 | 177 - 193 °C | 350 - 380 °F | |
LyondellBasell Petrothene® GA808093 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 808-093 is a broad molecular weight, linear low density polyethylene resin designed for use as a wire and cable insulation. An antioxidant package is added to ensure therm.. |
|||
Zone 2 | 177 - 193 °C | 350 - 380 °F | |
LyondellBasell Petrothene® HR92953 Medium Density Polyethylene ApplicationsPETROTHENE HR 92953 is a medium density polyethylene-based resin designed for use as jacketing for communications cable, including CATV and FOC. HR 92953 has a nominal carbon black cont.. |
|||
Zone 2 | 177 - 204 °C | 350 - 400 °F | |
LyondellBasell Petrothene® KR92717 High Density Polyethylene ApplicationsPETROTHENE KR 92717 is a high molecular weight, high density polyethylene-based compound designed for use in spacer cable insulation and cable jacketing applications. This black compoun.. |
|||
Zone 2 | 177 - 204 °C | 350 - 400 °F | |
LyondellBasell Petrothene® KR92828 High Density Polyethylene ApplicationsPETROTHENE KR 92828 is a high molecular weight, high density polyethylene-based compound designed for use in jacketing, conduit or wire insulation. KR 92828 contains a carbon black cont.. |
|||
Zone 2 | 177 - 193 °C | 350 - 380 °F | |
LyondellBasell Petrothene® PR92735 Linear Low Density Polyethylene ApplicationsPETROTHENE PR 92735 is a high molecular weight, linear low density-based compound designed for cable jacketing. PR 92735 contains a nominal carbon black content of 2.6% and antioxidant .. |
|||
Zone 2 | 177 - 204 °C | 350 - 400 °F | |
LyondellBasell Petrothene® LR590001 High Density Polyethylene ApplicationsPETROTHENE LR590001 is designed as primary insulation for telephone singles. LR590001 is a high density resin designed for low shrinkback after extrusion. Antioxidant has been added to e.. |
|||
Zone 2 | 177 - 204 °C | 350 - 400 °F | |
LyondellBasell Petrothene® LR590005 High Density Polyethylene ApplicationsPETROTHENE LR 5900-05 is a high density, high molecular weight resin designed for primary insulation for electronic cables. This resin exhibits low shrinkback after extrusion, contains .. |
|||
Zone 2 | 177 - 204 °C | 350 - 400 °F | |
LyondellBasell Petrothene® LR686001 High Density Polyethylene ApplicationsPETROTHENE LR686001 is designed for use as insulation for foam/skin telephone singles, and is a natural, expandable, high density polyethylene compound containing a chemical blowing agen.. |
|||
Zone 2 | 177 °C | 351 °F | Extrusion |
Lubrizol Estane® 58123 Thermoplastic Polyurethane Features: High moisture vapor transmission with low water swell and excellent low temperature and elasticity properties.Uses: Blown and flat die/cast film extrusion, injection molding and cable jack.. |
|||
Zone 2 | 177 °C | 351 °F | Extrusion |
Lubrizol ESTANE® 58245 Ether Based Thermoplastic Polyurethane Features: High moisture vapor transmission. Good low temperature properties and elasticity.Uses: Blown and flat die/cast film extrusion.Available in Americas, Europe, Middle East, Africa, India and .. |
|||
Zone 2 | 177 °C | 351 °F | Extrusion |
Lubrizol Estane® MVT 70AT3 Thermoplastic Polyurethane, Moisture Vapor Transmission Type: Estane® MVT 70AT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission with low water swell. Excellent low temperature properties and el.. |
|||
Zone 2 | 177 °C | 351 °F | Extrusion |
Lubrizol ESTANE® 54600 Ester Based Thermoplastic Polyurethane Features: Very good physical properties and chemical resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusion Available in Americas, Europe,.. |
|||
Zone 2 | 177 °C | 351 °F | Extrusion |
Lubrizol ESTANE® 54610 Ester Based Thermoplastic Polyurethane Features: Good physical properties and chemical resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusion.Available in Americas, Europe, Midd.. |
|||
Zone 2 | 177 °C | 351 °F | Extrusion |
Lubrizol ESTANE® 54640 Ether Based Thermoplastic Polyurethane Very good physical properties and hydrolysis resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusionAvailable in Americas, Europe, Middle E.. |
|||
Zone 2 | 177 - 193 °C | 351 - 379 °F | |
Clariant PEPR92735G5NAT LLDPE, 5% Glass Fiber, Chemically Coupled Data provided by Clariant Masterbatches |
|||
Zone 2 | 177 °C | 351 °F | Extrusion |
Lubrizol ESTANE® 58315 Ether Based Thermoplastic Polyurethane Features: Very good physical properties, hydrolysis resistance, low temperature performance and abrasion. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection.. |
|||
Zone 2 | 177 °C | 351 °F | Extrusion |
Lubrizol ESTANE® 58311 Ether Based Thermoplastic Polyurethane Features: Very good physical properties, hydrolysis resistance, low temperature performance and abrasion. Wide processing window for extrusion.Uses: Flat Die/Cast Film Extrusion, Profile ExtrusionAv.. |