Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0117 GPa | 1.70 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Sundex 790 Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0117 GPa | 1.70 ksi | Injection molded parts; DIN 53504 |
Huntsman IROGRAN® A 85 E 4719 TPU-Polyester Introduction: IROGRAN A 85 E 4719 is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offers a.. |
|||
300% Modulus | 0.0117 GPa | 1.70 ksi | Injection molded parts; DIN 53504 |
Huntsman IROGRAN® A 85 E 5719 FCM TPU-Polyester Introduction: IROGRAN A 85 E 5719 FCM is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offe.. |
|||
300% Modulus | 0.0117 - 0.0152 GPa | 1.70 - 2.20 ksi | ASTM D412 |
Huntsman KRYSTALFLEX® PE 399 Polyurethane Optical Aliphatic Film Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers |
|||
300% Modulus | 0.0117 GPa | 1.70 ksi | ASTM D412 |
SK Chemicals SKYTHANE® S180A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
300% Modulus | 0.0117 GPa | 1.70 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Sundex 790 Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0117 GPa | 1.70 ksi | ASTM D412 |
Lubrizol Estane® 2103-80AE Thermoplastic Polyurethane Elastomer Formerly PellethaneAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
300% Modulus | 0.0117 GPa | 1.70 ksi | ASTM D412 |
Lubrizol Estane® 2103-84AEN Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Contains UV Stabilizer, NSF Standard 61 certifiedAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pelletha.. |
|||
300% Modulus | 0.0117 GPa | 1.70 ksi | ASTM D412 |
Lubrizol ESTANE® 54640 Ether Based Thermoplastic Polyurethane Very good physical properties and hydrolysis resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusionAvailable in Americas, Europe, Middle E.. |
|||
300% Modulus | 0.0117 - 0.0138 GPa | 1.70 - 2.00 ksi | Secant; Conditioned 7 days at RT/50% RH; ASTM D638 |
AdvanSource Biomaterials ChronoFlex® C 55D Biodurable Medical Grade Polyurethane ChronoFlex® C is a family of premium polycarbonate aromatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® C medical-grade elastome.. |
|||
300% Modulus | 0.0117 GPa | 1.70 ksi | ASTM D412 |
Lubrizol ESTANE® 58311 Ether Based Thermoplastic Polyurethane Features: Very good physical properties, hydrolysis resistance, low temperature performance and abrasion. Wide processing window for extrusion.Uses: Flat Die/Cast Film Extrusion, Profile ExtrusionAv.. |