Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 21.0 kN/m | 120 pli | ISO 34-1 |
PolyOne OnFlex™ S HF 60A-3S1982 Thermoplastic Elastomer (TPE) OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu.. |
|||
Tear Strength | 21.0 kN/m @Temperature 21.0 °C |
120 pli @Temperature 69.8 °F |
Die C2 hr; ASTM D624 |
PolyOne Versalloy™ HC 9210-55N Thermoplastic Elastomer (TPE) Versalloy™ HC 9210-55N is a TPV alloy targeted for injection molding healthcare applications such as disposable medical items, syringe stoppers, and soft-touch overmolding onto surgical grips. Prod.. |
|||
Tear Strength | 21.0 kN/m @Temperature 21.0 °C |
120 pli @Temperature 69.8 °F |
Die C2 hr; ASTM D624 |
PolyOne Versalloy™ XL 9055X-9 Thermoplastic Elastomer (TPE) Versalloy™ XL 9055X-9 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Overmold Adhesion to Polypro.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | ASTM D624 |
Network Polymers Softflex® 0826 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Tear Strength | 21.0 kN/m | 120 pli | ASTM D624 |
PolyOne Dynaflex™ G2755-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2755-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Good Ozone and UV Stability - Overmold Adhesion to Polypro.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | Die B |
Momentive Performance Materials TUFELâ„¢ III 92656 Biocompatible Extrusion Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 40-LR-1 TPE Product Description: StarTUFF TF 40-LR-1 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | Fill/Transverse direction |
Saint-Gobain COHRlastic® 1010 General-Purpose Electrical-Grade Silicone Coated Fabric Description: Saint Gobain Performance Plastics CHR standard COHRlastic silicone coated fabrics, available from stock, have silicone rubber dispersion coated on both sides of fiberglass. They are thi.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | Warp/Longitudinal direction; ASTM D1000 |
Saint-Gobain COHRlastic® 1010 General-Purpose Electrical-Grade Silicone Coated Fabric Description: Saint Gobain Performance Plastics CHR standard COHRlastic silicone coated fabrics, available from stock, have silicone rubber dispersion coated on both sides of fiberglass. They are thi.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | Initial Tear Strength; ASTM D1004-93 |
Saint-Gobain Norprene® A-60-F Food Process Tubing Formulation Description: Norprene® Food Process Tubing, Formulation A-60-F: Formulated to withstand the high temperatures frequently occurring during food and beverage processing, Norprene® Food Process.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | Tensile Strength (Warp) |
Saint-Gobain Chemfab® 6 High-Performance PTFE-Coated Glass Description: Chemfab® High-Performance Series provides the highest level of PTFE content for superior surface smoothness, durability, and longer life. Use this product for the most demanding heat.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | Tensile Strength (Warp) |
Saint-Gobain Chemfab® 6 Primary PTFE-Coated Glass Description: Chemfab® Primary Series is an economical PTFE-coated glass fabric fiber used for belting, gaskets, and release sheets. It is designed as a lower cost alternative to our Description: .. |
|||
Tear Strength | 21.0 kN/m | 120 pli | Die C; ASTM D1004 |
Teknor Apex TEKRON® 4000-60 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tear Strength | 21.0 kN/m | 120 pli | |
Dow Corning HS II BASE & 10:1 CLAY CATALYST High strength silicone mold making rubber, suited for the art foundry industry that typically uses sulfur-based clays. HS II Base with HS II 10:1 Clay Catalyst is recommended for use with polyesters.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | |
Dow Corning SILASTIC® LS 5-8750 FLUOROSILICONE RUBBER 33 durometer, off-white, molding grade fluorosilicone base.Information provided by Dow Corning |
|||
Tear Strength | 21.0 kN/m | 120 pli | 73°C, Die C; ASTM D624 |
ExxonMobil Santoprene® 8281-65MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | ISO 34-B |
AlphaGary Evoprene™ 019 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | Parallel to flow; ISO 34-B |
AlphaGary Evoprene™ LF 6150 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | Tensile Strength (Warp) |
Saint-Gobain Chemfab® 5 Basic PTFE-Coated Glass Description: Chemfab® Basic Series products are low resin-content, non-porous, PTFE-coated fiberglass fabrics. Applications are spray shields, separator sheets, release sheets and protective barrie.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | Tensile Strength (Warp) |
Saint-Gobain Chemfab® 5 Porous PTFE-Coated Glass Description: Chemfab® Porous Series products are lightweight, highly porous materials commonly used as a release (non-stick) layer for composite curing, molding, and other processes that "off-gas.".. |
|||
Tear Strength | 21.0 kN/m | 120 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarCLEAR CLR-1045 TPE Product Description: StarCLEAR CLR-1045 is an easy processing TPE designed for injection molding. Soft and ultra clear TPEs specifically targeted to medical, consumer and sporting goods market. Feat.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® RT-3660 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerNaturalApplications:General PurposeInteriorMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingInformation provided by PolyOne.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® RT-3850E Thermoplastic Elastomer - SBC
(discontinued **) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | Tensile Strength (Warp) |
Saint-Gobain Chemfab® 5 Premium PTFE-Coated Glass Description: Chemfab® Premium Series combines a superior quality glass fabric with a high level of PTFE content. Description: Chemfab® Premium is an excellent multi-purpose fabric with a smooth, h.. |