Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 135 °C | 275 °F | |
Polikim ULPOLEN® 1000 UHMWPE, Flame Retardant For those producing flammable materials and in the mining industry, explosion and fire are major dangers. It is of vital importance that in conveyor belts and bunkers, lining material is flame retar.. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 2000 PE-UHMW, Q OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | ISO 3146 |
Okulen® 2000 PE-UHMW, SGB OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Melting Point | 135 °C | 275 °F | Internal method |
Polimeri Europa Eraclene® BC 86 High Density Polyethylene - Blow Molding Eraclene BC 86 is a high density polyethylene resin (HDPE) with antioxidants, suitable for blow molding application. It is especially recommended for the production of containers up to 20 liters.Er.. |
|||
Melting Point | 135 °C | 275 °F | Internal method |
Polimeri Europa Eraclene® FC 82 High Density Polyethylene - Blown Film Extrusion Eraclene FC 82 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Its broad molecular weight distribution and density successfully co.. |
|||
Melting Point | 135 °C | 275 °F | Internal method |
Polimeri Europa Eraclene® ML 70 U High Density Polyethylene - Injection Molding Eraclene ML 70 U is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.This grade has a narrow molecular weight distribution. It combin.. |
|||
Melting Point | 135 °C | 275 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Durapro® Truck Liners (ASTM Product Data Sheet) |
|||
Melting Point | 135 °C | 275 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP TIVAR® 88-2 ESD Black, Premium Lubricant Filled, Lower COF, Electro Static Dissipative Lining Material (ASTM Product Data Sheet) |
|||
Melting Point | 135 °C | 275 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
Quadrant EPP TIVAR® Burnguard PE-UHMW + flame retardant + other additives (ISO Data) TIVAR Burnguard is a PE-UHMW grade containing a very effective non-halogenated flame retardant. Specifically developed to improve the poor flammability behaviour of straight forward virgin polyethyl.. |
|||
Melting Point | 135 °C | 275 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
Quadrant EPP TIVAR® Dryslide PE-UHMW + internal lubricant + other additives (ISO Data) Thanks to the lubricant built into a PE-UHMW matrix with higher molecular weight, TIVAR DrySlide offers a lower coefficient of friction and enhanced wear and abrasion resistance than TIVAR 1000. The.. |
|||
Melting Point | 135 °C | 275 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
Quadrant EPP TIVAR® ECO PE-UHMW reprocessed (ISO Data) This grade, partially composed of reprocessed PE-UHMW material, has an overall lower property level than the virgin TIVAR 1000 and a lower cost. Compared with virgin PE 500, however, it has a much b.. |
|||
Melting Point | 135 °C | 275 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
Quadrant EPP TIVAR® Oil Filled PE-UHMW + oil (ISO Data) TIVAR Oil Filled is a self-lubricating PE-UHMW material in the real meaning of the word. Next to an enhanced wear resistance, the incorporated and evenly dispersed oil renders this material a consid.. |
|||
Melting Point | 135 °C | 275 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
Quadrant EPP TIVAR® SuperPlus PE-UHMW + specific additives (ISO Data) TIVAR SuperPlus is a wear optimised, partially cross-linked PE-UHMW material with extremely high degree of polymerisation for use in most demanding applications and environments. When used for drain.. |
|||
Melting Point | 135 °C | 275 °F | Internal method |
Polimeri Europa Eraclene® MS 80 High Density Polyethylene - Injection Molding Eraclene MS 80 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MS 80 shows a good balance between processability and mechanical pro.. |
|||
Melting Point | 135 °C | 275 °F | |
Mitsui Fybrel® E 620 Polyolefin Synthetic Pulp, Wet Processes
(discontinued **) Fybrel® (Polyolefin Synthetic Pulp) is a highly fibrillated fiber similar to wood pulp. There are three types available: Fybrel® E and Fybrel® UL, which are both made from polyethylene, and Type .. |
|||
Melting Point | 135 °C | 275 °F | |
Mitsui Fybrel® E 795 Polyolefin Synthetic Pulp, Dry Processes
(discontinued **) Fybrel® (Polyolefin Synthetic Pulp) is a highly fibrillated fiber similar to wood pulp. There are three types available: Fybrel® E and Fybrel® UL, which are both made from polyethylene, and Type .. |
|||
Melting Point | 135 °C | 275 °F | |
Mitsui Fybrel® E 990 Polyolefin Synthetic Pulp, Dry Processes
(discontinued **) Fybrel® (Polyolefin Synthetic Pulp) is a highly fibrillated fiber similar to wood pulp. There are three types available: Fybrel® E and Fybrel® UL, which are both made from polyethylene, and Type .. |
|||
Melting Point | 135 °C | 275 °F | Eutectic |
Indium Corp. Indalloy 75 Bismuth-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 135 °C | 275 °F | DIN 53736 |
Isoflon PEHD 500 High Density Polyethylene Products with excellent friction, anti-stick, abrasion and chemical inertia characteristicsVery good impact resistanceNo moisture regainProduct for the food industryInformation provided by Isoflon. |
|||
Melting Point | 135 °C | 275 °F | MTM 15902 |
LyondellBasell Adsylâ„¢ 5 C 37 F Polyolefin Description: Adsylâ„¢ 5 C 37 F is a new thermoplastic polyolefin which has been designed as a BOPP sealing layer material with exceptionally low sealing temperature. It features a high clarity an.. |
|||
Melting Point | 135 °C | 275 °F | TMA; MCI Method |
Mitsui APELâ„¢ APL6013T Cyclo Olefin Copolymer (COC) This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces.. |
|||
Melting Point | 135 - 145 °C | 275 - 293 °F | MQSA 111 |
Lubrizol Advanced Materials PEARLCOAT® Activa D118K Thermoplastic Polyurethane Elastomer PEARLCOAT® Activa D118K is a polycaprolactone copolyester based thermoplastic polyurethane of low hardness, supplied in form of natural pellets. This product gives an inherent “low gloss asp.. |
|||
Melting Point | 135 °C | 275 °F | |
Techmer ES HiFill® HDPE TM10 10% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Melting Point | 135 °C | 275 °F | |
Sanyo PELESTAT® 300 Antistatic Additive PELESTAT® alloy type anti-static additives are true IDP (Inherent Dissipative Polymers) that give permanent static dissipation performance to thermoplastics. Pelestat® comes tailored to a var.. |
|||
Melting Point | 135 °C | 275 °F | DSC |
Lubrizol Estane® 58123 Thermoplastic Polyurethane Features: High moisture vapor transmission with low water swell and excellent low temperature and elasticity properties.Uses: Blown and flat die/cast film extrusion, injection molding and cable jack.. |
|||
Melting Point | 135 - 137 °C | 275 - 279 °F | |
Addcomp PRIEX® Ionomer 45101 PP random copolymer Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce t.. |
|||
Melting Point | 135 °C | 275 °F | ISO 11357 |
Arkema Group Pebax® Rnew 35R53 SP 01 Polyether Block Amide (PEBA) Polyether block amide Pebax® 35R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV.. |
|||
Melting Point | 135 °C | 275 °F | DSC |
Lubrizol ESTANE® 58315 Ether Based Thermoplastic Polyurethane Features: Very good physical properties, hydrolysis resistance, low temperature performance and abrasion. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection.. |