Polymer Property : Drying Temperature = 104 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Drying Temperature 104 °C
219 °F
PolyOne Trilliant™ HC HC9820-0030 RS Natural Polyetheretherketone (PEEK)
The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead..
Drying Temperature 104 - 110 °C
220 - 230 °F
Polymer Resources PPX-FR3 Modified-PPO, V-1 Flame Retardant
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
Drying Temperature 104 - 110 °C
220 - 230 °F
Polymer Resources PPX-FR7 Modified-PPO, V-0 Flame Retardant
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 260F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
Drying Temperature 104 - 110 °C
220 - 230 °F
Polymer Resources PPX-G10HF Modified-PPO, 10% Glass Reinforced, High Flow
Modified-Polyphenylene Oxide, 10% Glass Reinforced, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf..
Drying Temperature 104 - 110 °C
220 - 230 °F
Polymer Resources PPX-GP1-[color]EN Modified PPO, Extrusion Grade with HDT of 265 F
Process: Extrusion Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Drying Temperature 104 - 110 °C
220 - 230 °F
Polymer Resources PPX-GP3-WR Modified-PPO, Wear Resistant
Modified-Polyphenylene Oxide, Wear Resistant, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water Absorption • Good Wear ResistanceProcess: Injection MoldingNotes: All physical, mechan..
Drying Temperature 104 - 110 °C
220 - 230 °F
Polymer Resources PPX-GP4-WR Modified-PPO, General Purpose, Wear Resistant
Modified-Polyphenylene Oxide, General Purpose, Wear Resistant, 215F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s..
Drying Temperature 104 - 110 °C
220 - 230 °F
Polymer Resources PPX-MF-FRG20 Modified-PPO, 40% Glass/Mineral Reinforced, Flame Retardant
Modified-Polyphenylene Oxide, 40% Glass/Mineral Reinforced, Flame RetardantFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanica..
Drying Temperature 104 °C
220 °F
Ravago Manufacturing Americas Hybrid S459 ABS + Polycarbonate Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Drying Temperature 104 - 110 °C

@Time 7200 - 14400 sec
220 - 230 °F

@Time 2.00 - 4.00 hour
Ravago Manufacturing Americas Hybrid S470H Acrylonitrile Butadiene Styrene + PC Alloy
Available in North America Flame Retardant RoHS Compliant UL File Number: E157012 Form: Pellets Processing Method: Injection Molding Information provided by Ravago
Drying Temperature 104 - 110 °C
220 - 230 °F
Average value: 107 °C Grade Count:5
Overview of materials for Polycarbonate/PET Polyester Blend, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend, Glass Reinforced". Each property range of values reported is minimum ..
Drying Temperature 104 °C
220 °F
RTP Company RTP 1503-40D Polyether-Ester Block Copolymer (TEEE/COPE), Glass Fiber
Drying Temperature 104 °C
219 °F
Lubrizol ESTANE® 58091 Ester Based Thermoplastic Polyurethane
Features: High stiffness TPU alloyUses: Flat Die/Cast Sheet Extrusion, Profile Extrusion and Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided b..
Drying Temperature 104 °C
219 °F
Lubrizol ESTANE® 58309 Ether Based Thermoplastic Polyurethane
Features: Good Physical Properties and Reduced Surface Tack.Uses: Flat Die/Cast Film and Blown Film Extrusion, Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInfo..
Drying Temperature 104 °C
219 °F
Lubrizol ESTANE® 58863 Ether Based Thermoplastic Polyurethane
Features: Good Elasticity – High melt flow for easy processingUses: Extrusion – Wire and cable, general extrusionAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provi..
Drying Temperature 104 °C
219 °F
Lubrizol ESTANE® 58866 Ether Based Thermoplastic Polyurethane
Features: Transparent flame retardant compoundUses: Extrusion – Wire and cable, Hose and tubeAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Drying Temperature 104 °C
219 °F
Lubrizol ESTANE® 58887 Ether Based Thermoplastic Polyurethane
Features: Excellent hydrolysis resistance, low temperature performance, clarity and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and blow molding; cab..
Drying Temperature 104 °C
219 °F
Lubrizol ESTANE® ETE50DS3 Ester Based Thermoplastic Polyurethane
Features: Excellent physical and low temperature properties with very good chemical resistance and wide processing window for extrusion.Uses: Flat die/cast film and tubing extrusion and Injection an..
Drying Temperature 104 °C
219 °F
Lubrizol ESTALOC® 59010 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane
Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas and AsiaInformation provided by Lubrizol
Drying Temperature 104 °C
219 °F
Lubrizol ESTALOC® 60204 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane
Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation pro..
Drying Temperature 104 °C
219 °F
Lubrizol ESTANE® 54640 Ether Based Thermoplastic Polyurethane
Very good physical properties and hydrolysis resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusionAvailable in Americas, Europe, Middle E..
Drying Temperature 104 °C
219 °F
Lubrizol ESTANE® 58142 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Drying Temperature 104 °C
219 °F
Lubrizol ESTANE® 58315 Ether Based Thermoplastic Polyurethane
Features: Very good physical properties, hydrolysis resistance, low temperature performance and abrasion. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection..
Drying Temperature 104 °C
219 °F
Lubrizol Estane® 58437 Thermoplastic Polyurethane
Type: Estane® 58437 is an 85A aromatic polyester-based thermoplastic polyurethane (TPU).Features: Excellent cold temperature properties and improved heat resistance.Uses: Blown and flat die/cast fi..
Drying Temperature 104 - 110 °C
220 - 230 °F
Polymer Resources PPX-G10 Modified PPO, 10% Glass Reinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Drying Temperature 104 - 110 °C
220 - 230 °F
Polymer Resources PPX-G30 Modified PPO, 30% Glass Reinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Drying Temperature 104 - 110 °C
220 - 230 °F
Polymer Resources PPX-GP7 Modified PPO, General Purpose with HDT of 300 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Drying Temperature 104 - 121 °C
219 - 250 °F
Average value: 115 °C Grade Count:7
Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass Filler". Each property range of values reported is minimum and ..
Drying Temperature 104 °C
219 °F
Lubrizol ESTANE® 58133 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUse: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and Asia Information provided by Lubrizol.
Drying Temperature 104 °C

@Time 7200 - 14400 sec
220 °F

@Time 2.00 - 4.00 hour
RTP Company RTP 2099 X 63578 C Polycarbonate/Polyester| (PC/PBT) Alloy, PC/PBT Alloy - UV Stabilized