Processing Properties Metric English Comments
Dew Point -40.0 °C
-40.0 °F
RTP Company RTP 4700 AR 15 TFE 15 Polytrimethylene Terephthalate (PTT), Aramid Fiber - PTFE Lubricated
Dew Point -40.0 °C
-40.0 °F
RTP Company RTP 4785 Polytrimethylene Terephthalate (PTT), Carbon Fiber
Dew Point <= -40.0 °C
<= -40.0 °F
Pre-drying
Celanese VECTRA C130 LCP, 30% Glass Reinforced  (Unverified Data**)
Has the same excellent balance of properties as A130 with higher temperature capability and easier flow. Slightly more dimensional stability in vapor phase soldering than A130. Suitable for some i..
Dew Point <= -40.0 °C
<= -40.0 °F
Pre-drying
Celanese VECTRA E130G LCP, 30% Glass Reinforced  (Unverified Data**)
30% glass fiber filled/low injection pressureInformation provided by Celanese
Dew Point <= -40.0 °C
<= -40.0 °F
Pre-drying
Celanese VECTRA E463i LCP, 40% Mineral / Glass Reinforced  (Unverified Data**)
40% glass/mineral filled exellent flow, low warpage, high heat resistance.Information provided by Celanese
Dew Point <= -40.0 °C
<= -40.0 °F
Pre-drying
Celanese VECTRA MT1305 LCP, 15% Glass Reinforced  (Unverified Data**)
Provides easier flow than MT1310. Slightly tougher, but may warp slightly more than MT1310 in some parts. 15% glass reinforced.15% Glass fiber reinforcedA three-zone screw evenly divided into feed,..
Dew Point <= -40.0 °C
<= -40.0 °F
Pre-drying
Celanese VECTRA MT4310 LCP, 30% Medical Technology  (Unverified Data**)
Highest temperature capability, easiest flow. Suitable where very thin walls are required. Used for broad range of SMT applications, with minimal dimensional change. 30% glass filled.30% glass fiber..
Dew Point -40.0 °C
-40.0 °F
Average value: -40.0 °C Grade Count:3
Overview of materials for Nylon 12, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
Dew Point -40.0 °C
-40.0 °F
RTP Company RTP 1104 M 15 BLK Polyethylene Terephthalate (PET), 25% Glass Fiber - 15% Mineral
Dew Point -40.0 °C
-40.0 °F
RTP Company RTP 1105 BLK Polyethylene Terephthalate (PET), Glass Fiber
Dew Point -40.0 °C
-40.0 °F
RTP Company RTP 2000 HC A Polyester Alloy Medical Cleaner Resistant - UV Stabilized
RTP 2000 HC series are polyester alloys designed to withstand the aggressive cleaners used to disinfect medical equipment
Dew Point -40.0 °C
-40.0 °F
Lubrizol ESTANE® 58137 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUse: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Dew Point -40.0 °C
-40.0 °F
Lubrizol ESTANE® 58238 Ester Based Thermoplastic Polyurethane
Features: Highly Elastic Compound and Good Recovery for a Rubber-Like CharacterUses: Flat Die/Film Extrusion and Blown Film and Injection Molding and Profile ExtrusionAvailable in Americas, Europe, ..
Dew Point -40.0 °C
-40.0 °F
Lubrizol Estane® 58246 Thermoplastic Polyurethane
Features: High stiffness grade with excellent chemical and oil resistance.Uses: Flat Die/Cast Film Extrusion and Injection Molding.Available in Americas, Europe, Middle East, Africa, India and AsiaI..
Dew Point -40.0 °C
-40.0 °F
RTP Company RTP 2302 C Rigid Thermoplastic Polyurethane (RTPU), Glass Fiber
Dew Point -40.0 °C
-40.0 °F
RTP Company RTP 2381 A Rigid Thermoplastic Polyurethane (RTPU), Carbon Fiber
Dew Point -40.0 °C
-40.0 °F
RTP Company RTP 2383 C Rigid Thermoplastic Polyurethane (RTPU), Carbon Fiber
Dew Point -40.0 °C
-40.0 °F
RTP Company RTP 2505 A TFE 15 Rigid Thermoplastic Polyurethane (RTPU), Glass Fiber - PTFE Lubricated
Dew Point -40.0 °C
-40.0 °F
RTP Company RTP 281 F Nylon 12 (PA), Carbon Fiber
Dew Point -40.0 - -30.0 °C
-40.0 - -22.0 °F
Lubrizol Estane® 54643 Polyester-Based Thermoplastic Polyurethane
Feature: Excellent flame retardant properties, matt surface appearance and low surface friction and transparent spherical pelletsUses: Melt roll coated fabrics and calenderingAvailable in Americas, ..
Dew Point -40.0 °C
-40.0 °F
RTP Company RTP 2099 X 124790 B Bio-Based Polylactic Acid (PLA); Impact Modified - Mineral - Fast-Cycle Nucleator - 68% Renewable Resource Content
Nucleated for high heat exposure.  For detailed processing information regarding this, see the PLA Molding Guide on the RTP Company website.
Dew Point -40.0 °C
-40.0 °F
RTP Company RTP 2099 X 126218 A Bio-Based Polylactic Acid (PLA); Impact Modified - 94% Renewable Resource Content
For detailed processing information, see the PLA Molding Guide on the RTP Company website.
Dew Point -40.0 °C
-40.0 °F
AdvanSource Biomaterials ChronoFlex® AL 55D Biodurable Medical Grade Polyurethane
ChronoFlex® AL is a family of premium polycarbonate aliphatic biodurable thermoplastic polyurethane elastomers developed by  AdvanSource Biomaterials Corporation. ChronoFlex® AL medical-grade el..
Dew Point -40.0 °C
-40.0 °F
AdvanSource Biomaterials ChronoFlex® AL 65D Biodurable Medical Grade Polyurethane
ChronoFlex® AL is a family of premium polycarbonate aliphatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® AL medical-grade elas..
Dew Point -40.0 °C
-40.0 °F
AdvanSource Biomaterials ChronoFlex® C 55D Biodurable Medical Grade Polyurethane
ChronoFlex® C is a family of premium polycarbonate aromatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® C medical-grade elastome..
Dew Point -40.0 °C
-40.0 °F
Lubrizol ESTANE® 58211 Ether Based Thermoplastic Polyurethane
Features: Halogenated flame retardant compound – High hardnessUses: Extrusion – wire and cable jacketing and general extrusion where flame retardant propertied are requiredAvailable in Americas, E..
Dew Point -40.0 °C
-40.0 °F
RTP Company RTP 4499 X 113529 A High Temperature Nylon (HTN) Glass Fiber - Flame Retardant - Halogen Free
Preliminary Data Sheet
Dew Point -40.0 °C
-40.0 °F
RTP Company RTP 2099 X 126210 BLACK Bio-Based Polylactic Acid (PLA); PC-PLA Blend - 32% Renewable Resource Content - Additional 49% Post Consumer Content
For detailed processing information, see the PLA Molding Guide on the RTP Company website.
Dew Point -40.0 °C
-40.0 °F
RTP Company RTP 2305 A Rigid Thermoplastic Polyurethane (RTPU), Glass Fiber
Dew Point -40.0 °C
-40.0 °F
RTP Company RTP 4701 Polytrimethylene Terephthalate (PTT), Glass Fiber