Polymer Property : Specific Gravity = 1.13 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
NuSil MED-6385 Low Consistency Elastomer - Unrestricted Medical Use
Description: Low consistency elastomers (LCEs) are useful alternatives to liquid silicone rubber (LSR) and high consistency rubber (HCR) for end users who need a low viscosity elastomer which provid..
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Polymax® Maxelast® A9760 TPE, ABS/PC Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform..
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
SABIC Innovative Plastics Cycoloy® CY200FC PC+ABS
High flow PC+ABS material designed for local Pacific Automotive applications
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
SABIC Innovative Plastics Cycoloy® IP1000 PC+ABS (Asia Pacific)
IP1000 is a high impact PC/ABS blend developed for the automotive instrument panel business.
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
SABIC Innovative Plastics Cycoloy® LG9020 PC+ABS
Low Gloss Cycoloy. Available only in natural, to be custom color concentrated and UV stabilized at the molding press.
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D 792
RTP Company RTP 4000 ET-1001 L Polyphthalamide (PPA), Impact Modified - Lubricated
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
SABIC Innovative Plastics Cycoloy® CP8930 PC+ABS (Asia Pacific)
High heat, PC/ABS for automotive electro plating applications, excellent balance in flow/impact
Specific Gravity 1.13 g/cc
1.13 g/cc
DAM; ASTM D792
DuPont Performance Polymers Zytel® 7304 NC010 Nylon 6  (Unverified Data**)
Zytel® 7304 NC010 is a medium viscosity, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
RTP Company RTP 200F TFE 20  Nylon 12 (PA 12) PTFE 20%  (discontinued **)
PTFE 20%Comments:PTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for thi..
Specific Gravity 1.13 g/cc

@Temperature 23.0 °C
1.13 g/cc

@Temperature 73.4 °F
ASTM D792
Kingfa MAC-601 UV PC/ABS Alloy
Features:Excellent balance propertiesHigh impact strengthGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic partsComputer and accessoriesHou..
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
LG Chemical LUMID GP1300A(W) PA6, High Viscosity
Feature: Injection Molding, PA6, High ViscosityApplication: Automotive PartsCAS No. 25038-54-4Information provided by LG Chemical
Specific Gravity 1.13 g/cc
1.13 g/cc
Lucite International Elvacite ® 2927 Acrylic Resin
Lucite International has developed novel polymer chemistry which delivers Elvacite® thermoplastic acrylic resins with controlled molecular architecture and enables the coatings formulator to achi..
Specific Gravity 1.13 g/cc

@Temperature 23.0 °C
1.13 g/cc

@Temperature 73.4 °F
ASTM D792
Kingfa MAC-551 PC/ABS Alloy
Features:Excellent balance propertiesGood low temperature impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile license platePower toolComp..
Specific Gravity 1.13 g/cc
1.13 g/cc
Momentive Performance Materials Addisilâ„¢ 442 E Healthcare Extrusion Grade Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
SABIC Innovative Plastics PREVEX VGAX PPE+PS
Improved productivity and reliability. Nonchlorinated, nonbrominated flame retardant. 180F HDT.
Specific Gravity 1.13 g/cc
1.13 g/cc
Shin-Etsu Silicones KEG-2001-70A/B Fast Curing LIMS Silicone Rubber
ShinEtsu KEG200170 is a very fast cure liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. The viscosity of KEG20..
Specific Gravity 1.13 g/cc
1.13 g/cc
23°C; ASTM D792
Teknor Apex Flexalloy® 9900-60 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Oil Resistant, Ultra High MWUses- Footwear, Tubing, Gaskets, Tools (Power/Others), Hose, Wire and ..
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Teknor Apex MONPRENE® MP 2790 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Chase Plastics CP Pryme® N300HSL (DAM) Nylon 6 (Utility Grade), Heat Stabilized, Internally Lubricated
Information provided by Chase Plastics.
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
A. Schulman POLYTROPE™ TPP 530 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 530 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp..
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
A. Schulman SCHULAMID® 66 MV3H Unreinforced Nylon 6/6
Information provided by A. Schulman.
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
A. Schulman POLYBLAK™ 3209 Superior Black Color Concentrate, 40% Carbon Black Based In Polypropylene
DescriptionPOLYBLAK® Black 3209 is a superior black color concentrate containing 40% carbon black in polypropylene. This masterbatch is designed to provide good opacity and a regular blue underton..
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Eastman Neostar FN007 Elastomer
Neostar FN007 elastomer is the third in Eastman’s series of tough, clear, durable copolyester ethers. Though originally designed for use in the profile and automotive markets, this innovative copol..
Specific Gravity 1.13 g/cc
1.13 g/cc
15/15°C
ChevronTexaco Heavy Duty Coolant
No requirement for precharge dose of SCAEasy maintenanceExcellent pitting protection for wet sleeve cylinder linersEffective corrosion protection for aluminum, brass, cast iron, steel, solder, and c..
Specific Gravity 1.13 g/cc
1.13 g/cc
catalyzed with Moldmaster Blue
ACC QM 2128 QSI Quantum Silicones 28 Durometer Condensation Cure Moldmaking Material
QM 2128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch..
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Asahi Kasei Thermylene® P6-30FG-0632 30% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Asahi Kasei Thermylene® P6-30FG-0640 30% Glass Fiber Reinforced, Heat and Copper
Information provided by Asahi Thermofil
Specific Gravity 1.13 g/cc
1.13 g/cc
catalyzed with Moldmaster Blue
ACC QM 2125 QSI Quantum Silicones 25 Durometer Condensation Cure Moldmaking Material
QM 2125 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch..
Specific Gravity 1.13 g/cc
1.13 g/cc
Mixed; TM R050-16
Resinlab® EP1238 Acrylic / Epoxy Hybrid Adhesive
Resinlab™ EP1238 is a two part acrylic / epoxy hybrid adhesive designed for bonding metals and plastics. It cures quickly at room temperature to a tough, semi-rigid material. It has good wetting to..
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Loxim 400 00HB Nylon 6,6
Information provided by Loxim Industries