Kraton® D2109 DS-W (SBS) Compound

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene/Butadiene/Styrene (SBS)
Manufacturer Kraton
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraton® D2109 DS-W (SBS) Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Kraton D2109 DS-W is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form identified: Kraton D2109 DS-W - supplied as a dense, white pellet Region: North America, Europe, Asia Pacific, Japan, and South AmericaApplications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Footwear; and Impact ModificationInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.915 - 0.945 g/cc
0.915 - 0.945 g/cc
BAM 1014
Linear Mold Shrinkage, Flow 0.025 - 0.027 cm/cm
0.025 - 0.027 in/in
Melt Flow 14 - 24 g/10 min

@Load 5.00 kg,
Temperature 200 °C
14 - 24 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 40 - 50
40 - 50
Value of product compression molded 120°C; BAM 1003
Tensile Strength 3.45 MPa
500 psi
Machine Direction, typical properties Injection molded plaques, Die C; ASTM D412
4.83 MPa
701 psi
Transverse Direction, typical properties Injection molded plaques, Die C; ASTM D412
Elongation at Break 550 %
550 %
Machine Direction, typical properties Injection molded plaques, Die C; ASTM D412
800 %
800 %
Transverse Direction, typical properties Injection molded plaques, Die C; ASTM D412
100% Modulus 0.00103 GPa
0.149 ksi
Transverse Direction, typical properties Injection molded plaques, Die C; ASTM D412
0.00138 GPa
0.200 ksi
Machine Direction, typical properties Injection molded plaques, Die C; ASTM D412
300% Modulus 0.00172 GPa
0.249 ksi
Transverse Direction, typical properties Injection molded plaques, Die C; ASTM D412
0.00207 GPa
0.300 ksi
Machine Direction, typical properties Injection molded plaques, Die C; ASTM D412
Tear Strength 21.9 kN/m
125 pli
Transverse Direction, typical properties Injection molded plaques, Die C; ASTM D412
26.3 kN/m
150 pli
Machine Direction, typical properties Injection molded plaques, Die C; ASTM D412
Processing Properties Metric English Comments
Rear Barrel Temperature 171 - 182 °C
340 - 360 °F
Middle Barrel Temperature 177 - 193 °C
350 - 380 °F
Front Barrel Temperature 188 - 199 °C
370 - 390 °F
Mold Temperature 10.0 - 37.8 °C
50.0 - 100 °F
Injection Pressure 3.549 - 4.928 MPa
514.7 - 714.7 psi
Back Pressure 0.276 - 0.414 MPa
40.0 - 60.0 psi