Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.023 - 0.027 cm/cm
0.023 - 0.027 in/in
ASTM D955
Polymax® Maxelast® P2950T TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Linear Mold Shrinkage, Flow 0.023 - 0.027 cm/cm
0.023 - 0.027 in/in
ASTM D955
PolyOne Geon™ Vinyl Flexible A6500 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne
Linear Mold Shrinkage, Flow 0.023 - 0.027 cm/cm
0.023 - 0.027 in/in
ASTM D955
PolyOne Geon™ Vinyl Flexible A65M0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne
Linear Mold Shrinkage, Flow 0.025 - 0.027 cm/cm
0.025 - 0.027 in/in
ASTM D955
PolyOne Edgetek® 5209 Black 30 A 1 Acetal (POM) Copolymer
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Linear Mold Shrinkage, Flow 0.025 - 0.027 cm/cm
0.025 - 0.027 in/in
ASTM D955
PolyOne Edgetek® 5209 Natural 1 Acetal (POM) Copolymer
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Linear Mold Shrinkage, Flow 0.025 - 0.027 cm/cm
0.025 - 0.027 in/in
ASTM D955
PolyOne Edgetek® 5230 Natural 1 Acetal (POM) Copolymer
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Linear Mold Shrinkage, Flow 0.023 - 0.027 cm/cm
0.023 - 0.027 in/in
ASTM D955
PolyOne Geon™ Vinyl Flexible B5500 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Linear Mold Shrinkage, Flow 0.023 - 0.027 cm/cm
0.023 - 0.027 in/in
ASTM D955
PolyOne Geon™ Vinyl Flexible B550B Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Linear Mold Shrinkage, Flow 0.025 - 0.027 cm/cm
0.025 - 0.027 in/in
Kraton® D2104 DI-N (SBS) Compound
Description: Kraton D2104 DI-N is an easy processing, general purpose material designed for a wide variety of applications. It is supplied from North America in the physical form identified: D2104 D..
Linear Mold Shrinkage, Flow 0.025 - 0.027 cm/cm
0.025 - 0.027 in/in
Kraton® D2109 DS-N (SBS) Compound
Description: Kraton D2109 DS-N is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form..
Linear Mold Shrinkage, Flow 0.025 - 0.027 cm/cm
0.025 - 0.027 in/in
Kraton® D2109 DS-W (SBS) Compound
Description: Kraton D2109 DS-W is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form..
Linear Mold Shrinkage, Flow 0.023 - 0.027 cm/cm
0.023 - 0.027 in/in
LATI Latan 13E71 POM
Polyoxymethylene (POM). Toughened. Medium viscosity. Good elongation and impact resistance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided ..
Linear Mold Shrinkage, Flow 0.023 - 0.027 cm/cm
0.023 - 0.027 in/in
LATI Latan 3E71 POM
Polyoxymethylene (POM). Toughened. High viscosity. Good elongation and impact resistanceAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by ..
Linear Mold Shrinkage, Flow 0.024 - 0.027 cm/cm

@Thickness 3.20 mm
0.024 - 0.027 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Valox® 337 PBT
Low temperature impact PBT. Automotive applications: underhood power distribution boxes and covers.
Linear Mold Shrinkage, Flow 0.021 - 0.027 cm/cm

@Thickness 3.20 mm
0.021 - 0.027 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Valox® IQ3001 PBT (Asia Pacific)
Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications.
Linear Mold Shrinkage, Flow 0.021 - 0.027 cm/cm

@Thickness 3.20 mm
0.021 - 0.027 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Valox® IQ3001 PBT (Europe-Africa-Middle East)
Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications.
Linear Mold Shrinkage, Flow 0.021 - 0.027 cm/cm

@Thickness 3.20 mm
0.021 - 0.027 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Valox® IQ3001 PBT
Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications.
Linear Mold Shrinkage, Flow 0.021 - 0.027 cm/cm

@Thickness 3.20 mm
0.021 - 0.027 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Valox® V3004 PBT (Asia Pacific)
Unfilled PBT modified with elastomer. Targeted for flexible hinge, automotive connectors, film applications.
Linear Mold Shrinkage, Flow 0.024 - 0.027 cm/cm

@Thickness 4.00 mm
0.024 - 0.027 in/in

@Thickness 0.157 in
E2P method
Eurostar Star L POM D84 POM, Injection Molded
Star L POM D84 is a PTFE/Proprietary Additive Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar.