Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 182 - 193 °C | 360 - 380 °F | |
Polymer Resources AC-G10 Acetal Copolymer, 10% Glass Reinforced Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Middle Barrel Temperature | 182 - 193 °C | 360 - 380 °F | |
Polymer Resources AC-G25 Acetal Copolymer, 25% Glass Reinforced Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Middle Barrel Temperature | 177 - 193 °C | 350 - 380 °F | |
Kraton® D2104 DI-N (SBS) Compound Description: Kraton D2104 DI-N is an easy processing, general purpose material designed for a wide variety of applications. It is supplied from North America in the physical form identified: D2104 D.. |
|||
Middle Barrel Temperature | 177 - 193 °C | 350 - 380 °F | |
Kraton® D2109 DS-N (SBS) Compound Description: Kraton D2109 DS-N is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Middle Barrel Temperature | 177 - 193 °C | 350 - 380 °F | |
Kraton® D2109 DS-W (SBS) Compound Description: Kraton D2109 DS-W is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Middle Barrel Temperature | 177 - 193 °C | 350 - 380 °F | |
Teknor Apex Flexalloy® 9100-65 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather.. |
|||
Middle Barrel Temperature | 177 - 193 °C | 350 - 380 °F | |
Teknor Apex Flexalloy® 9300-60 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, Oil Resistant, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather R.. |
|||
Middle Barrel Temperature | 171 - 193 °C | 340 - 380 °F | |
Tempia Polylactic acid (PLA) Resin A bio-degradable plastic, Polylactic acid (PLA) is made from corn. Products produced are compostable within 45 – 120 days. The degradation process of the item is temperature, humidity and thicknes.. |
|||
Middle Barrel Temperature | 179 - 193 °C | 355 - 380 °F | |
ExxonMobil Santoprene® 8201-60 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
Middle Barrel Temperature | 166 - 193 °C | 330 - 380 °F | |
Clariant CA9000NAT` Acetal Copolymer Data provided by Clariant Masterbatches |
|||
Middle Barrel Temperature | 188 - 193 °C | 370 - 380 °F | |
Clariant OMAN698583 Thermoplastic Polyurethane, Halogen Free, Flame Retardant Aromatic Polyether BasedData provided by Clariant Masterbatches |
|||
Middle Barrel Temperature | 179 - 193 °C | 355 - 380 °F | |
ExxonMobil Santoprene® 8211-60 Thermoplastic Elastomer
(discontinued **) A soft, colorable, non-hygroscopic, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance .. |