Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 26.3 kN/m | 150 pli | 73°F; ASTM D624 |
Advanced Elastomer Systems Santoprene® 8281-65 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Tear Strength | 26.3 kN/m | 150 pli | ASTM D624 |
PolyOne Dynaflex™ G7660-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7660-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible D7000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 26.3 kN/m | 150 pli | Die B, post cured- 4 hours at 177°C; ASTM D624 |
Multibase C6-250 PERKADOX PD-50S Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 26.3 kN/m | 150 pli | Initial Tear Strength |
Saint-Gobain CHR® 2975-8R Glass-Silicone Backing Silicone Adhesive Pressure Sensitive Tape Description: Silicone glass provides temperature resistance from -85°F to +500°F (-62°C to +260°C) and exceptional tensile strength and abrasion resistance. Applications include thermal .. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Initial Tear Strength |
Saint-Gobain CHR® SG15-05(R) High Performance Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Initial Tear Strength |
Saint-Gobain CHR® SG25-06(R) Primary Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Initial Tear Strength |
Saint-Gobain CHR® SG26-06(R) Primary Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Tensile Strength (Warp) |
Saint-Gobain Chemfab® TCN® 1590 Leno Weave Nomex/Fiberglass Belting Material Description: General Notes on Saint Gobain Chemfab® TCN® Open Mesh Belting Products:TCN belting products are PTFE coated Nomex®, a high-temperature polyamide fiber that maintains its struct.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Trouser; ASTM D470 |
Lubrizol ESTANE® 58226 Ester Based Thermoplastic Polyurethane Features: Excellent physical properties, good chemical resistance and enhanced hydrolysis resistance. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | ASTM D624 |
Diamond Polymers Softflex® SF 0450 Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Die B, Silicone Property; ASTM D624 |
Arlon 32580R020 0.020" (0.508 mm) Uncured Silicone Rubber on Polyester Film Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmAppearance: Red silicone gum on polymer linerThis data represents typical values for the production.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Die B, Silicone Property; ASTM D624 |
Arlon 32580R035 0.035" (0.889 mm) Uncured Silicone Rubber on PET Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. .. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Side 2, Silicone Property; ASTM D624 |
Arlon 51586R052 0.052" (1.32 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothInterleave: Polyethylene.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Side 2 Silicone Property; ASTM D624 |
Arlon 51588R015 0.015" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 1 Layer 2: Uncured Silicone RubberSide 1 Layer 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: LDPETh.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Silicone Property; ASTM D624 |
Arlon 55589R032 0.034" (0.864 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 FiberglassAppearance: Red silicone gum and rubber on fiberglass This.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Side 2, Silicone Property; ASTM D624 |
Arlon 56586R026 0.027" (0.686 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: Red silicone gum and rubber on fiberglass clo.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Die B, Silicone Property; ASTM D624 |
Arlon 99580R010 0.010" (0.254 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction: Interleave: FEP FilmSide 1: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassFlexible heater substrateAppearance: Red, High viscosity gum on release linersThis data repres.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Die B, Silicone Property; ASTM D624 |
Arlon 32580R060 0.060" (1.52 mm) Uncured Silicone Rubber on PET Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. .. |
|||
Tear Strength | 26.3 kN/m | 150 pli | ASTM D624C |
3M 5300 Motor Lead Splicing Kits 3M Motor Lead Splicing Kits 5300 Series are a series of kits designed for splicing motor lead cables to incoming feeder cables. The kits accommodate the follow splice confiations:Pigtails (stub) con.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Side 2, Silicone Property; ASTM D624 |
Arlon 49586B010 0.0115" (0.292 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1681 FiberglassSide 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mater.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Die C; ASTM D624C-73 |
3M 8430-18 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Die C; ASTM D624-73 |
3M 8453 Cable Accessory Sealing Kits 3M Cable Accessory Sealing Kits provide a reliable means of sealing the jacket end of power cables where elbows or other cable accessories are installed. The seal is accomplished with use of tubular.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Layer 1, Silicone Property; ASTM D624 |
Arlon 55589G028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Green silicone gum and rubber on fiberglass Th.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Die C; ASTM D624C-73 |
3M SJ-1A Cold Shrink Jacket Kits 3M™ SJ series Cold Shrink™ Splice Jacket Kits are a series of open ended, tubular, rubber sleeves that combined with Scotch™ 2228 Rubber Mastic Tape provide a sealed jacket over cable splice inst.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Die B; Silicone Property; ASTM D624 |
Arlon 32580R030 0.030" Uncured Silicone Rubber on PET Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberCarrier: 0.005" PETThis data represents typical values for the production material and should not be used as mate.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Trosuer; ASTM D470 |
Lubrizol ESTANE® 58315 Ether Based Thermoplastic Polyurethane Features: Very good physical properties, hydrolysis resistance, low temperature performance and abrasion. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Die C; ASTM D624 |
Kraton® G7720 GI-N (SEBS) Compound Description: Kraton G7720 GI-N is an easy processing, general purpose 57 Shore a hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® q-GUARD® 112 Insulation Jacketing Description: q-GUARD® is a thermally durable and fire-safe composite developed specifically for use with removable and reusable insulation systems. Based upon PTFE fluorocarbon resins and fiberglas.. |