Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 3.549 - 4.928 MPa | 514.7 - 714.7 psi | |
Kraton® D2104 DI-N (SBS) Compound Description: Kraton D2104 DI-N is an easy processing, general purpose material designed for a wide variety of applications. It is supplied from North America in the physical form identified: D2104 D.. |
|||
Injection Pressure | 3.549 - 4.928 MPa | 514.7 - 714.7 psi | |
Kraton® D2109 DS-N (SBS) Compound Description: Kraton D2109 DS-N is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Injection Pressure | 3.549 - 4.928 MPa | 514.7 - 714.7 psi | |
Kraton® D2109 DS-W (SBS) Compound Description: Kraton D2109 DS-W is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |