Arkema Group Pebax® MX 1283 Polyether Block Amide (PEBA) (Dry)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyether Block Amide (PEBA)
Manufacturer Arkema
Trade Name Pebax®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Pebax® MX 1283 Polyether Block Amide (PEBA) (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
POLYETHER BLOCK AMIDE (PEBA) Supersoft grade (hardness 72 shore A) Modified 2533SN01 Applications: sport (tennis shoes parts)ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
Water Absorption 1.1 %
1.1 %
Moisture Absorption at Equilibrium 0.30 %
0.30 %
Humidity Absorption
Melt Flow 14 g/10 min

@Load 1.00 kg,
Temperature 235 °C
14 g/10 min

@Load 2.20 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 72
72
Tensile Strength, Yield 1.80 MPa

@Strain 50.0 %
261 psi

@Strain 50.0 %
50 mm/min
Tensile Modulus 0.00700 GPa
1.02 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
Low Temp
NB
NB
Charpy Impact, Notched NB
NB
Low Temp
NB
NB
Thermal Properties Metric English Comments
Melting Point 135 °C
275 °F
10°C/min
Glass Transition Temp, Tg -50.0 °C
-58.0 °F
10°C/min
Electrical Properties Metric English Comments
Electrical Resistivity 9.12e+11 ohm-cm
9.12e+11 ohm-cm
Surface Resistance 2.73e+12 ohm
2.73e+12 ohm
Dielectric Strength 40.0 kV/mm
1020 kV/in
Dissipation Factor 0.000428

@Frequency 1e+6 Hz
0.000428

@Frequency 1e+6 Hz
0.00043

@Frequency 100 Hz
0.00043

@Frequency 100 Hz
Comparative Tracking Index 600 V
600 V