Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00172 GPa | 0.249 ksi | Transverse Direction, typical properties Injection molded plaques, Die C; ASTM D412 |
Kraton® D2109 DS-N (SBS) Compound Description: Kraton D2109 DS-N is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
300% Modulus | 0.00172 GPa | 0.249 ksi | Transverse Direction, typical properties Injection molded plaques, Die C; ASTM D412 |
Kraton® D2109 DS-W (SBS) Compound Description: Kraton D2109 DS-W is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
300% Modulus | 0.00172 GPa | 0.249 ksi | |
Kraton® D4141 (SBS) Linear Block Copolymer (SBS) styrene-butadiene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact .. |
|||
300% Modulus | 0.00172 GPa @Time 7200 sec |
0.250 ksi @Time 2.00 hour |
Die C; ASTM D412 |
STAR Thermoplastic Alloys & Rubbers StarGrip GP 45-9000 TPE Product Description: StarGrip GP 45-9000 is an easy processing TPE designed for injection molding and this particular class of TPE material with excellent grip properties. Features:Soft TouchRubbery.. |
|||
300% Modulus | 0.00172 GPa | 0.250 ksi | ASTM D 412 |
CPT C-Flex® R70-091 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |