Mechanical Properties Metric English Comments
100% Modulus 0.00138 GPa
0.200 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N990 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00138 GPa
0.200 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with Cumar P-10 Plasticizer
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
100% Modulus 0.00138 GPa
0.200 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, Hardness 52A
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
100% Modulus 0.00138 GPa
0.200 ksi
ASTM D412
Mearthane Durethaneâ„¢ S DS-660A Solid Polyurethane Elastomer
MDI backbone: ester.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, ..
100% Modulus 0.00138 GPa
0.200 ksi
Machine Direction, typical properties Injection molded plaques, Die C; ASTM D412
Kraton® D2109 DS-N (SBS) Compound
Description: Kraton D2109 DS-N is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form..
100% Modulus 0.00138 GPa
0.200 ksi
Machine Direction, typical properties Injection molded plaques, Die C; ASTM D412
Kraton® D2109 DS-W (SBS) Compound
Description: Kraton D2109 DS-W is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form..
100% Modulus 0.00138 GPa
0.200 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with Cumar P-10 Plasticizer
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
100% Modulus 0.00138 GPa
0.200 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, Hardness 52A
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
100% Modulus 0.00138 GPa
0.200 ksi
ASTM D412
Teknor Apex TEKRON® 4000-60 Thermoplastic Elastomer
Information provided by Teknor Apex Company
100% Modulus 0.00138 GPa
0.200 ksi
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 10.0 PHR Wacker HDK N20 Filler
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed ..
100% Modulus 0.00138 GPa
0.200 ksi
ASTM D 412
CPT C-Flex® R70-085 Clear Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
100% Modulus 0.00138 GPa
0.200 ksi
ASTM D412
Elastocon TPE Technologies Elastocon® STK40B Thermoplastic Elastomer
Elastocon® STK40B is a black thermoplastic elastomer that has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK40B is well s..
100% Modulus 0.00138 GPa
0.200 ksi
ASTM D412; ISO 37
Advanced Polymer Alloys DuraGrip™ DGR 6040 NCEHT Thermoplastic Elastomer (TPE)
DuraGrip® DGR 6040NCEHT is a general purpose Thermoplastic Elastomer (TPE) designed to process easily in injection molding and extrusion. It features excellent soft touch feel with improved surface..
100% Modulus 0.00138 GPa
0.200 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N774 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00138 GPa
0.200 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N990 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00138 GPa
0.200 ksi
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, 10.0 PHR Wacker HDK N20 Filler
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed ..
100% Modulus 0.00138 GPa
0.200 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N774 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..