Processing Properties Metric English Comments
Rear Barrel Temperature 166 - 182 °C
331 - 360 °F
PolyOne Versaflex™ HC 2110-57B Thermoplastic Elastomer (TPE)
Versaflex™ HC 2110-57B is a TPE designed for use in the healthcare industry offering low stiction and good compression set. New Product. Commercial specifications have not been established. - Bonds..
Rear Barrel Temperature 166 - 182 °C
331 - 360 °F
PolyOne Versaflex™ HC MT555 Thermoplastic Elastomer (TPE)
Versaflex™ HC MT555 is an easy processing material designed for applications where FDA compliance and medical testing is required. - Excellent Colorability - Soft TouchRear: 340 - 360F Center: 380 ..
Rear Barrel Temperature 166 - 182 °C
331 - 360 °F
PolyOne Versaflex™ VDT 4132 Thermoplastic Elastomer (TPE)
Versaflex™ VDT 4132 is designed to create vibration damping. - Excellent Vibration DampingRear = 350-370F Middle = 375-400F Front = 375-400F Nozzle = 365-380F Screw speed = 100-500rpmPurge thorough..
Rear Barrel Temperature 171 - 182 °C
340 - 360 °F
Polymer Resources ABS-FR Flame Retardant ABS
Flame Retardant Acrylonitrile Butadiene StyreneFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch..
Rear Barrel Temperature 171 - 182 °C
340 - 360 °F
Polymer Resources ABS-FR-[color]-UV Flame Retardant ABS, UV-stabilized
Flame Retardant Acrylonitrile Butadiene Styrene, UV-stabilizedFeatures: • Flame Retardant • Self Extinguishing • Good UV ResistanceProcess: Injection MoldingNotes: All physical, mechanical and..
Rear Barrel Temperature 171 - 182 °C
340 - 360 °F
Polymer Resources ABS-FR1 ABS, Flame Retardant
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Rear Barrel Temperature 171 - 182 °C
340 - 360 °F
PTS Trilac® FR3800 Flame Retardant ABS Resin, RoHS Compliant
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 171 - 182 °C
340 - 360 °F
PTS Trilac® FR3800-V Flame Retardant ABS Resin, RoHS Compliant
Contains UV absorber.Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 160 - 182 °C
320 - 360 °F
PolyOne Dynalloy™ 8900-30 Thermoplastic Elastomer (TPE)
Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen..
Rear Barrel Temperature 160 - 182 °C
320 - 360 °F
PolyOne Dynalloy™ 8900-80 Thermoplastic Elastomer (TPE)
Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen..
Rear Barrel Temperature 166 - 182 °C
331 - 360 °F
PolyOne Dynaflex™ G7736-1 Thermoplastic Elastomer (TPE)
Dynaflex™ G7736-1 is a general purpose compound designed to provide easy processing and a good surface finish. - Good Aesthetics - Good Ozone/UV Stability - High Flow for Thin-Wall Parts - Overmold..
Rear Barrel Temperature 160 - 182 °C
320 - 360 °F
PolyOne Dynalloy™ 8900-60 Thermoplastic Elastomer (TPE)
Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen..
Rear Barrel Temperature 177 - 182 °C
350 - 360 °F
Green Dot Terratek® SC 50 Polypropylene - Wheat Starch Biocomposite
Terratek® SC 50 is a proprietary blend of wheat starch and polypropylene for injection molding applications. SC 50 contains 50% wheat starch by weight, however, a range of properties can be achie..
Rear Barrel Temperature 177 - 182 °C
350 - 360 °F
Green Dot Terratek® SC 65 Polypropylene - Wheat Starch Biocomposite
Terratek® SC 65 is a proprietary blend of wheat starch and polypropylene for injection molding applications. SC 65 contains 65% wheat starch by weight, however, a range of properties can be achie..
Rear Barrel Temperature 177 - 182 °C
350 - 360 °F
Green Dot Terratek® WC 100300 Polypropylene - Pine Fiber Composite
Terratek® WC 100300 is a proprietary blend of pine wood fiber and reprocessed polypropylene for injection molding applications. WC 100300 contains 30% wood fiber by weight, however, a range of pr..
Rear Barrel Temperature 171 - 182 °C
340 - 360 °F
LTL Color Compounds ColorFast® FRA202 General Purpose ABS
General purpose V0/5VA-rated ABSAll information provided by LTL Color Compounders, Inc.
Rear Barrel Temperature 171 - 182 °C
340 - 360 °F
LTL Color Compounds ColorFast® FRA203 ABS
Business machinery V0 ABS with excellent indoor light stabilityAll information provided by LTL Color Compounders, Inc.
Rear Barrel Temperature 171 - 182 °C
340 - 360 °F
LTL Color Compounds ColorFast® FRA204 ABS
High gloss, excellent impact ABS, V0/5VA-ratedAll information provided by LTL Color Compounders, Inc.
Rear Barrel Temperature 171 - 182 °C
340 - 360 °F
LTL Color Compounds ColorFast® FRA205 ABS
Flame-retarded V0, high gloss ABS with superior UV stabilityAll information provided by LTL Color Compounders, Inc.
Rear Barrel Temperature 171 - 182 °C
340 - 360 °F
Kraton® D2104 DI-N (SBS) Compound
Description: Kraton D2104 DI-N is an easy processing, general purpose material designed for a wide variety of applications. It is supplied from North America in the physical form identified: D2104 D..
Rear Barrel Temperature 171 - 182 °C
340 - 360 °F
Kraton® D2109 DS-N (SBS) Compound
Description: Kraton D2109 DS-N is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form..
Rear Barrel Temperature 171 - 182 °C
340 - 360 °F
Kraton® D2109 DS-W (SBS) Compound
Description: Kraton D2109 DS-W is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form..
Rear Barrel Temperature 166 - 182 °C
330 - 360 °F
Star Plastics ABS450FR Molding Grade ABS
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 149 - 182 °C
300 - 360 °F
Star Plastics ABSFR1 Molding Grade ABSFR
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 149 - 182 °C
300 - 360 °F
Star Plastics ABSFR2 Molding Grade ABS
Information provided by Star Plastics, Inc.
Rear Barrel Temperature 160 - 182 °C
320 - 360 °F
Clariant CA9000NAT` Acetal Copolymer
Data provided by Clariant Masterbatches