Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00207 GPa | 0.300 ksi | Measured on films cast from a solution in toluene; ASTM D412 |
Kraton® D1171 P (SIBS) Linear Triblock Copolymer Description: Kraton D1171 P is a clear, linear triblock copolymer based on styrene, butadiene and isoprene with a polystyrene content of 19%. It is supplied from North America in the form: Kraton D1.. |
|||
300% Modulus | 0.00207 GPa | 0.300 ksi | Machine Direction, typical properties Injection molded plaques, Die C; ASTM D412 |
Kraton® D2109 DS-N (SBS) Compound Description: Kraton D2109 DS-N is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
300% Modulus | 0.00207 GPa | 0.300 ksi | Machine Direction, typical properties Injection molded plaques, Die C; ASTM D412 |
Kraton® D2109 DS-W (SBS) Compound Description: Kraton D2109 DS-W is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
300% Modulus | 0.00207 GPa | 0.300 ksi | ASTM D412 |
Kraton® G7705 GI-B (SEBS) Compound Description: Kraton G7705 GI-B is an easy processing, general purpose 44 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
300% Modulus | 0.00207 GPa | 0.300 ksi | ASTM D412 |
Kraton® G7705 GI-N (SEBS) Compound Description: Kraton G7705 GI-N is an easy processing, general purpose 44 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
300% Modulus | 0.00207 GPa | 0.300 ksi | ASTM D412 |
Kraton® D1133 K (SBS) Linear Block Copolymer Description: Kraton D1133 K is a clear, linear triblock copolymer based on styrene and butadiene, with a polystyrene content of 36%. It is supplied from North America in the physical form identified.. |
|||
300% Modulus | 0.00207 GPa | 0.300 ksi | Estimated value; ASTM D412 |
Kraton® D1133 K (SBS) Linear Triblock Copolymer Description: Kraton D1133 K is a clear, linear triblock copolymer based on styrene and butadiene, with a polystyrene content of 36%. It is supplied from North America in the physical form identified.. |
|||
300% Modulus | 0.00207 GPa | 0.300 ksi | ASTM D412 |
Teknor Apex MONPRENE® MP 2750 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
300% Modulus | 0.00207 GPa | 0.300 ksi | ASTM D412 |
Teknor Apex MONPRENE® MP 2760 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
300% Modulus | 0.00207 GPa | 0.300 ksi | ASTM D412 |
Teknor Apex MONPRENE® MP 2840M Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
300% Modulus | 0.00207 GPa | 0.300 ksi | ASTM D412 |
Teknor Apex MONPRENE® MP 2850E Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
300% Modulus | 0.00207 GPa | 0.300 ksi | ASTM D412 |
Advanced Polymer Alloys DuraGrip™ 6140 NC Thermoplastic Elastomer DuraGrip® 6140NC is an enhanced bonding and adhesion grade Thermoplastic Elastomer (TPE) designed for injection molding and extrusion processes. It will bond well with polycarbonate, polycarbonate .. |