Material Notes:
For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc.
Physical Properties Metric English Comments
Density 9.92 g/cc
0.358 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 95
95
Tensile Strength, Ultimate 723 MPa
105000 psi
Tensile Strength, Yield 655 MPa
95000 psi
Modulus of Elasticity 248 GPa
36000 ksi
Flexural Modulus 1.137 GPa
164.9 ksi
Thermal Properties Metric English Comments
CTE, linear 6.50 µm/m-°C

@Temperature 20.0 °C
3.61 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.260 J/g-°C
0.0621 BTU/lb-°F
Thermal Conductivity 140 W/m-K
972 BTU-in/hr-ft²-°F
Melting Point 1080 - 2610 °C
1980 - 4730 °F
Solidus 1080 °C
1980 °F
Liquidus 2610 °C
4730 °F
Component Elements Properties Metric English Comments
Copper, Cu 15 %
15 %
Molybdenum, Mo 85 %
85 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000616 ohm-cm
0.00000616 ohm-cm
(28% IACS)