Kingfa JH960 6111 Non-halogenated Flame Retardant PC/ABS Alloy

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Kingfa Sci. & Tech. Co.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kingfa JH960 6111 Non-halogenated Flame Retardant PC/ABS Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent mechanical propertiesHigh heat resistanceChemical resistance, hydrolysis resistanceGood paint adhesionHigh flow ability, suit for gas assistant moldingApplications:LCD cabinetPDP TV setOA cabinetNotebook computer and transformerChargerMobile CD and DVDPower toolsMobile phone enclosureInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc

@Temperature 23.0 °C
1.19 g/cc

@Temperature 73.4 °F
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm

@Temperature 23.0 °C
0.0050 - 0.0070 in/in

@Temperature 73.4 °F
ASTM D955
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 260 °C
12 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength at Break >= 55.0 MPa
>= 7980 psi
50mm/min; ASTM D638
Elongation at Break >= 50 %
>= 50 %
50mm/min; ASTM D638
Flexural Strength 85.0 MPa
12300 psi
2mm/min; ASTM D790
Flexural Modulus 2.60 GPa
377 ksi
2mm/min; ASTM D790
Izod Impact, Notched 3.80 J/cm

@Thickness 3.20 mm,
Temperature -10.0 °C
7.12 ft-lb/in

@Thickness 0.126 in,
Temperature 14.0 °F
ASTM D256
5.00 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
9.37 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 102 °C

@Thickness 6.40 mm
216 °F

@Thickness 0.252 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C

@Thickness 6.40 mm
194 °F

@Thickness 0.252 in
ASTM D648
Flammability, UL94 5VB

@Thickness 1.60 mm
5VB

@Thickness 0.0630 in
5VA

@Thickness 3.20 mm
5VA

@Thickness 0.126 in
Electrical Properties Metric English Comments
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
ASTM D257
Dielectric Strength 19.0 kV/mm
483 kV/in
1.6mm; ASTM D149
Processing Properties Metric English Comments
Processing Temperature <= 270 °C
<= 518 °F
Rear Barrel Temperature 220 - 250 °C
428 - 482 °F
Start Point: 215°C
Middle Barrel Temperature 230 - 255 °C
446 - 491 °F
Start Point: 225°C
Front Barrel Temperature 235 - 265 °C
455 - 509 °F
Start Point: 235°C
Melt Temperature 230 - 250 °C
446 - 482 °F
Start Point: 230°C
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Start Point: 60°C
Drying Temperature 80.0 - 90.0 °C

@Time 7200 - 14400 sec
176 - 194 °F

@Time 2.00 - 4.00 hour
Pre-dry
Back Pressure 0.300 - 0.700 MPa
43.5 - 102 psi
Descriptive Properties Value Comments
Injection Speed 50-80%