Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 220 °C | 428 °F | |
NYCOA 534H PA 6 high viscosity, heat stabilized, nucleated nylon for tubing, sheet, film and moldingInformation provided by NYCOA, Inc. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 230°C |
Kingfa PBT-T30 30% Mineral Filled PBT Features:Excellent size stabilityLow tendency to wrapLow abrasionGood surfaceApplications:Injection moldingApplication partsE & E partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 230°C |
Kingfa UTPBT-HB Toughened PBT Features:High impactExcellent size stabilityEasy processingApplications:Injection moldingSwitch partsKeyboard keysE & E partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Rear Barrel Temperature | 220 - 235 °C | 428 - 455 °F | Injection Molding |
LG Chemical LUPOS GP2300 ABS+GF30%, General Purpose Feature: Injection Molding, ABS+GF30%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-54-7, 9003-56-9 and 65997-17-3Information provided by LG Chemical |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical LUPOY GP5106F PC/ABS+GF10%, Flame Retardance Description: Injection Molding, PC/ABS+GF10%, Flame RetardanceApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG Chemical |
|||
Rear Barrel Temperature | 220 - 260 °C | 428 - 500 °F | |
LG Chemical LUPOY HR-5006A Heat Resistant PC/ABS Alloy, Unreinforced, Weather Resistant Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 235°C |
Kingfa MAC-451 UV Modified PC/ABS Alloy Features:Excellent balance propertiesGood weather resistanceGood impact strengthGood processing propertiesSuit for electro-platingApplications:Injection moldingAutomobile license plateWater tank cov.. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 235°C |
Kingfa MAC-451PG Electroplating PC/ABS Alloy Features:Excellent balance propertiesGood impact strengthGood processing propertiesSuit for electro-platingApplications:Injection moldingAutomobile license plateWater tank coverComputer and accessor.. |
|||
Rear Barrel Temperature | 220 - 235 °C | 428 - 455 °F | Start Point: 230°C |
Kingfa MAC-501DY Modified PC/ABS Alloy Features:Excellent balance propertiesGood low temperature impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile license platePower toolComp.. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 230°C |
Kingfa MAC-701 PC/ABS Alloy Features:Excellent balance propertiesHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic p.. |
|||
Rear Barrel Temperature | 220 - 245 °C | 428 - 473 °F | Start Point: 230°C |
Kingfa MAC-751 PC/ABS Alloy Features:Excellent balance propertiesSuper high impact strengthGood electro-plating propertiesGood processing propertiesGood glossApplications:Injection moldingAutomobile instrument panelElectrical .. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 230°C |
Kingfa PBT-R0N Flame Retardant PBT Features:Flame retardantGood chemical resistanceOutstanding surfaceEasy processingHigh impactApplications:Injection moldingConnectors, terminal blocksRelay, switchBobbinsPlugsE & E partsInformation .. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 235°C |
Kingfa PBT-RG002 Flame Retardant PBT Features:Flame retardantGood chemical resistanceOutstanding surfaceEasy processingHigh impactApplications:Injection moldingConnectors, terminal blocksRelay, switchBobbinsPlugsE & E partsInformation .. |
|||
Rear Barrel Temperature | 220 - 235 °C | 428 - 455 °F | Injection Molding |
LG Chemical LUPOS GP2200 ABS+GF20%, General Purpose Feature: Injection Molding, ABS+GF20%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7 and 65997-17-3Information provided by LG Chemical |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical LUPOY GN5001RF PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Good FlowApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical.. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical LUPOY GP1000LG PC, Transparent Description: Injection Molding, PC, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsInformation provided by LG Chemical |
|||
Rear Barrel Temperature | 220 - 230 °C | 428 - 446 °F | |
Solvay Technyl® C 206 Nylon 6, EH0 Unreinforced Plyamide PA6, standard for fast cycling, for injection molding.Technyl C 206 has high fluidity and good mold release, favored by a high crystallization rate. It is specially suitable f.. |
|||
Rear Barrel Temperature | 220 - 225 °C | 428 - 437 °F | |
Solvay Technyl Starâ„¢ S 218 V30 30% Glass Reinforced Nylon 6 Heat stabilized, low viscosity, injection grade.Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Rear Barrel Temperature | 220 - 250 °C | 428 - 482 °F | Aft-1. Region Temperature |
Tisan TISESTER® 30% Glass Fiber Reinforced and heat Stabilized Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Rear Barrel Temperature | 220 - 250 °C | 428 - 482 °F | Aft-1. Region Temperature |
Tisan TISESTER® 30% Glass Fiber Reinforced, Flame Retardant (V0). Heat Stabilized. Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Rear Barrel Temperature | 220 - 250 °C | 428 - 482 °F | Aft-1. Region Temperature |
Tisan TISESTER® 30% Glass Fiber Reinforced, Impact Resistance and Heat Stabilized ISI Stab. Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Aft-1. Region Temperature |
Tisan TISLAMID® 6 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Aft-1. Region Temperature |
Tisan TISLAMID® 6 Flame Retardant (V0) Heat Stabilized Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Aft-1. Region Temperature |
Tisan TISLAMID® 6 UNR Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Rear Barrel Temperature | 220 - 230 °C | 428 - 446 °F | Zone 1 |
Eurostar Staramide BST01 PA6, Impact Modified, Injection Molded BST01 is an Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Rear Barrel Temperature | 220 - 265 °C | 428 - 509 °F | |
Beijing Chemical Industry KAIFA® MN301-M30 Nylon 66 Resin Mineral filled, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Rear Barrel Temperature | 220 - 265 °C | 428 - 509 °F | |
Beijing Chemical Industry KAIFA® MN301-G0 Nylon 66 Resin High flame retardant, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical KEYFLEX BT S5035 Ester Type TPE Description: Injection Molding, TPC-ET, Airbag Cover Deployment, Medium Modulus, Black ColorApplication: Airbag Cover (DAB, PAB, KAB, SAB)CAS: 37282-12-5, 24968-12-5 and 1333-86-4Information provide.. |