Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 19.0 kV/mm @Frequency 100 Hz |
483 kV/in @Frequency 100 Hz |
|
Multibase TPSiV™ 3010-50A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | ASTM D149 |
Solvay Specialty Polymers Amodel® A-1115 HS Polyphthalamide (PPA) Resin, 15% Glass Reinforced, Dry As Molded
AMODEL A-1115 HS resin is a 15% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, and high tensile strength. Excellent cre.. |
|||
Dielectric Strength | 19.0 - 43.0 kV/mm | 483 - 1090 kV/in | Average value: 25.5 kV/mm Grade Count:8 |
Overview of materials for Acetal Copolymer, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values .. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | ASTM D149 |
Kolon Kocetal® VT701 Modified Grade Acetal Copolymer
(discontinued **) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Dielectric Strength | 19.0 - 35.0 kV/mm | 483 - 889 kV/in | Average value: 26.6 kV/mm Grade Count:12 |
Overview of materials for Nylon 6-3 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | ASTM D149 |
Kingfa JH710 G10 Flame Retardant & 10% Glass Reinforced PC Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc.. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | ASTM D149 |
Kolon KOCETAL® EL304 Toughened Grade Acetal Resin Flexible grade. Applications: Flexible products. Information provided by API-Kolon. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | ASTM D149 |
Kolon KOCETAL® GB705 Glass Bead Reinforced Acetal Resin Glass bead added, improved dimensional stability. Applications: Products for high stiffness, dimensional precision. Information provided by API-Kolon. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | ASTM D149 |
Kolon KOCETAL® GF105 G/F Reinforced Acetal Resin Glass fiber reinforced, improved stiffness. Applications: Products for high stiffness, improved fatigue properties. Information provided by API-Kolon. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | ASTM D149 |
Kolon KOCETAL® K500 Standard Grade Acetal Resin General injection molding grade. Easy flow grade for hard-to fill molds and mechanical thin-wall parts.Applications: General injection molding products.Information provided by API-Kolon. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | ASTM D149 |
Kolon KOCETAL® TC701 Mineral Reinforced Acetal Resin Talc reinforced, improved dimensional stability. Applications: Products for high stiffness, dimensional precision. Information provided by API-Kolon. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 1.00 mm |
483 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical LUMID GP1300AP PA6, Plasticized Feature: Injection Molding, PA6, PlasticizedApplication: Automotive PartsInformation provided by LG Chemical |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 1.00 mm |
483 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical LUMID HI1102A(W) PA6, High Impact Feature: Injection Molding, PA6, High ImpactApplication: H/Lamp Screw MountingCAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 3.20 mm |
483 kV/in @Thickness 0.126 in |
ASTM D149 |
Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AE-4133 is a 33% glass reinforced, hot-water moldable polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Good Chemical Resistance; Good Cree.. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | IEC 60243-1 |
Polyplastics Tepcon M25 Acetal-copolymer (POM), High Viscosity Information provided by PolyPlastics. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | IEC 60243-1 |
Polyplastics Tepcon M320 Acetal-copolymer (POM), High Fluidity, High Cycle Information provided by PolyPlastics. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | ASTM D149 |
Covestro Prism® CM-200 Polyurethane Solid RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and o.. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 3.20 mm |
483 kV/in @Thickness 0.126 in |
Short time; ASTM D149 |
Daikin POLYFLON MG-1030 PTFE 15% Glass Fiber Filled Molding Powder 15% glass fiber filled. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Available in all forms (e.g. bearings, gaskets, valve seats,.. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 3.20 mm |
483 kV/in @Thickness 0.126 in |
Short time; ASTM D149 |
Daikin POLYFLON MG-1431 PTFE 15% Glass Fiber and 5% MoS2 Filled Molding Powder 15% glass fiber and 5% MoS2 filled. High wear resistance, good electrical properties, low friction, high creep resistance.Applications: Mechanical and electrical service (e.g. split-curled bearings.. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 3.20 mm |
483 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
Eurostar Staramide RF006SXS PA66, 30% Glass Fiber Filled, Injection Molded Staramide RF006SXS is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006HS)Information provided by Eurostar. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 1.60 mm |
483 kV/in @Thickness 0.0630 in |
ASTM D149 |
E-Polymers SEPAZ® K140HF 40% Glass Fiber Reinforced Low Flash, High Flow PPS Resin Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit.. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | IEC 60243-1 |
Celanese CELANEX 3400-2 PBT, 40% Glass Reinforced Celanex 3400-2 is a general purpose, 40% glass reinforced polybutylene terephthalate that offers a good combination of mechanical, electrical, and thermal properties. This grade provides outstanding.. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | IEC 60243-1 |
Celanese Celanex® 3409HR PBT, 40% Glass Reinforced Celanex 3409HR is a non-lubricated, 40% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and processability.To avoid hydrolytic degra.. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 3.17 mm |
483 kV/in @Thickness 0.125 in |
50% R.H.; ASTM D149 |
Celanese Celanex® 5200 Polyester (PBT), 15% Glass-Fiber Good surface smoothnessInformation provided by Celanese Corporation. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 2.00 mm |
483 kV/in @Thickness 0.0787 in |
ASTM D149 |
Beijing Ranger Chem PBT-201-G10 291 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 2.00 mm |
483 kV/in @Thickness 0.0787 in |
ASTM D149 |
Beijing Ranger Chem PBT-MFC-G0 FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 2.00 mm |
483 kV/in @Thickness 0.0787 in |
ASTM D149 |
Beijing Ranger Chem PBT-201-G0 272 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 2.00 mm |
483 kV/in @Thickness 0.0787 in |
ASTM D149 |
Beijing Ranger Chem PBT-201-G0 291 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | IEC 60243-1 |
Polyplastics Duracon® M90-71 Acetal Co-polymer (POM), Heat resistance DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | IEC 60243-1 |
Polyplastics Duracon® HP25X Acetal Co-polymer (POM), High stiffness, High viscosity DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |