Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.300 MPa | 43.5 psi | |
Premix Thermoplastics PRESEAL® TPE 6080 General Description:PRESEAL® TPE 6080 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It can also be used as conductors or in grounding.. |
|||
Back Pressure | 0.300 MPa | 43.5 psi | Moulding a 6 gram (shot weight) gasket with a 50 ton injection moulding machine having a screw diameter of 25[mm] |
Premix Thermoplastics PRETHERM TPE 1075 Thermoplastic Elastomer, Boron Nitride / SEBS compound PRETHERM TPE 1075 is a thermoplastic elastomer based highly thermally conductive compound intended primarily for heat dissipation. It can be used as gap filler between processor and heat sink or co-.. |
|||
Back Pressure | 0.300 - 0.500 MPa | 43.5 - 72.5 psi | |
PolyOne Bergamid™ XP6042701 Polyamide 6 (Nylon 6) Injection Speed: 50 to 80% Holding Time: 3 to 9 sec Injection Time: 1 to 3.5 sec Cycle Time: 18 to 60 secInformation provided by PolyOne |
|||
Back Pressure | 0.300 - 1.00 MPa | 43.5 - 145 psi | |
Kingfa JH710 G10 Flame Retardant & 10% Glass Reinforced PC Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc.. |
|||
Back Pressure | 0.300 - 1.00 MPa | 43.5 - 145 psi | |
Kingfa JH710 G15 Flame Retardant & 15% Glass Fiber Reinforced PC Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc.. |
|||
Back Pressure | 0.300 - 1.00 MPa | 43.5 - 145 psi | |
Kingfa JH720 G15 15% Glass Fiber Reinforced PC Features:Excellent balance propertiesHigh mechanical propertiesHigh stiffnessGood size stabilityGood surfaceApplications:Imaging equipment shellOA body frameElectrical equipmentComputer plug partsIn.. |
|||
Back Pressure | 0.300 - 1.00 MPa | 43.5 - 145 psi | |
Kingfa JH720 G30 30% Glass Fiber Reinforced PC Features:High mechanical strengthGood size stabilityLow tendency to warpGood surfaceSuitable for exact moldingApplications:Imaging equipment shellOA body frameElectrical equipmentComputer plug parts.. |
|||
Back Pressure | 0.300 - 1.00 MPa | 43.5 - 145 psi | |
Kingfa JH720 G50 50% Glass Fiber Reinforced PC Features:Excellent balance propertiesSuper high stiffnessHigh hardnessGood size stabilitySuper high mechanical strengthApplications:Imaging equipment shellOA body frameElectrical equipmentComputer p.. |
|||
Back Pressure | 0.300 - 0.700 MPa | 43.5 - 102 psi | |
Kingfa JH960 6100 Non-halogenated Flame Retardant PC/ABS Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent mechanical propertiesChemical resistanceHydrolysis resistanceDrop down resistantSuper high flow ability, suit for thin w.. |
|||
Back Pressure | 0.300 - 0.700 MPa | 43.5 - 102 psi | |
Kingfa JH960 6111 Non-halogenated Flame Retardant PC/ABS Alloy Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent mechanical propertiesHigh heat resistanceChemical resistance, hydrolysis resistanceGood paint adhesionHigh flow ability,.. |
|||
Back Pressure | 0.300 - 0.700 MPa | 43.5 - 102 psi | |
Kingfa LONOY 1200 PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Back Pressure | 0.300 - 0.700 MPa | 43.5 - 102 psi | |
Kingfa LONOY 1600 PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Back Pressure | 0.300 - 0.700 MPa | 43.5 - 102 psi | |
Kingfa LONOY 3010 Glass Fiber Reinforced PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingElectric and electronic partsBusiness machine cabinetGarden to.. |
|||
Back Pressure | 0.300 - 1.00 MPa | 43.5 - 145 psi | |
Kingfa MAC-451 PC/ABS Alloy Features:Excellent balance propertiesGood impact strengthGood processing propertiesSuit for electro-platingApplications:Injection moldingHousehold applianceAutomobile interior/exterior trim partsTel.. |
|||
Back Pressure | 0.300 - 1.00 MPa | 43.5 - 145 psi | |
Kingfa MAC-601 DY Modified 60/40 PC/ABS Alloy Features:Excellent balance propertiesHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelPower toolComputer and acce.. |
|||
Back Pressure | 0.300 - 1.00 MPa | 43.5 - 145 psi | |
Kingfa MAC-751 HF PC/ABS Alloy Features:Excellent balance propertiesSuper high impact strengthGood electro-plating propertiesGood processing propertiesGood glossApplications:Injection moldingAutomobile instrument panelElectrical .. |
|||
Back Pressure | 0.300 - 1.00 MPa | 43.5 - 145 psi | |
Kingfa PC-S609 Toughened PC Features:Good mechanical propertiesSuper high impact strengthGood weather resistanceHigh glossGood processing propertiesStress cracking propertiesApplications:OA and IT partsAutomobile accessoriesEl.. |
|||
Back Pressure | 0.300 - 1.00 MPa | 43.5 - 145 psi | |
Kingfa PC-S923 Modified PC Features:Excellent balance propertiesGood weather resistanceHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelElec.. |
|||
Back Pressure | 0.300 - 0.700 MPa | 43.5 - 102 psi | |
Kingfa JH710 G30 Flame Retardant & 30% Glass Fiber Reinforced PC Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc.. |
|||
Back Pressure | 0.300 - 0.700 MPa | 43.5 - 102 psi | |
Kingfa LONOY 2100 LT PC/PET Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Back Pressure | 0.300 - 0.700 MPa | 43.5 - 102 psi | |
Kingfa LONOY 2200 HT PC/PET Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Back Pressure | 0.300 - 1.00 MPa | 43.5 - 145 psi | |
Kingfa MAC-501DY Modified PC/ABS Alloy Features:Excellent balance propertiesGood low temperature impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile license platePower toolComp.. |
|||
Back Pressure | 0.300 - 1.00 MPa | 43.5 - 145 psi | |
Kingfa MAC-551 PC/ABS Alloy Features:Excellent balance propertiesGood low temperature impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile license platePower toolComp.. |
|||
Back Pressure | 0.300 - 1.00 MPa | 43.5 - 145 psi | |
Kingfa PC-WT01 Weather Resistance PC Features:Excellent balance propertiesGood weather resistanceHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelElec.. |
|||
Back Pressure | 0.300 - 0.703 MPa | 43.5 - 102 psi | Injection |
Alliance Polymers Viprene™ G40D-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G40D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Back Pressure | 0.300 - 0.703 MPa | 43.5 - 102 psi | Injection |
Alliance Polymers Viprene™ G45D-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G45D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Back Pressure | 0.300 - 1.30 MPa | 43.5 - 189 psi | Injection |
Alliance Polymers Zythane™ 5050D Thermoplastic Polyurethane Elastomer Zythane™ 5050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Back Pressure | 0.300 - 1.30 MPa | 43.5 - 189 psi | Injection |
Alliance Polymers Zythane™ 6050D Thermoplastic Polyurethane Elastomer Zythane™ 6050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Back Pressure | 0.300 - 1.30 MPa | 43.5 - 189 psi | Injection |
Alliance Polymers Zythane™ 7050D Thermoplastic Polyurethane Elastomer Zythane™ 7050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Back Pressure | 0.300 - 0.703 MPa | 43.5 - 102 psi | Injection |
Alliance Polymers Viprene™ G40D-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G40D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |