Polymer Property : Back Pressure = 0.700 MPa Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Back Pressure 0.300 - 0.700 MPa
43.5 - 102 psi
PTS PBT-6630 30% Glass Filled
PBT6630 is an injection molding grade, with 30% glass fiber reinforced, high heat stability, and electrical properties, easy to process. It is widely used in automotive, home appliance, Electrical i..
Back Pressure 0.300 - 0.700 MPa
43.5 - 102 psi
Kingfa JH720 G10 10% Glass Fiber Reinforced PC
Features:High mechanical strengthGood size stabilityGood surfaceSuitable for exact moldingApplications:Exact mechanism partsPrinter, photocopies, scanner cabinetComputer plug partsCD-ROM, DVDElectri..
Back Pressure 0.300 - 0.700 MPa
43.5 - 102 psi
Kingfa JH960 6100 Non-halogenated Flame Retardant PC/ABS
Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent mechanical propertiesChemical resistanceHydrolysis resistanceDrop down resistantSuper high flow ability, suit for thin w..
Back Pressure 0.300 - 0.700 MPa
43.5 - 102 psi
Kingfa JH960 6111 Non-halogenated Flame Retardant PC/ABS Alloy
Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent mechanical propertiesHigh heat resistanceChemical resistance, hydrolysis resistanceGood paint adhesionHigh flow ability,..
Back Pressure 0.300 - 0.700 MPa
43.5 - 102 psi
Kingfa JH960 6300 Non-halogenated Flame Retardant PC/ABS Alloy
Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent balance propertiesHigh heat resistanceGood chemical resistanceGood hydrolysis resistanceSuit for paint and electo-platin..
Back Pressure 0.300 - 0.700 MPa
43.5 - 102 psi
Kingfa JH960 6610 Non-halogenated Flame Retardant PC/ABS Alloy
Features:Halogen free flame retardant, V-0/1.5mmExcellent balance propertiesHigh heat resistanceGood chemical resistanceGood hydrolysis resistanceSuit for paint and electo-platingDrop down resistanc..
Back Pressure 0.300 - 0.700 MPa
43.5 - 102 psi
Kingfa JH960 HT10 Non-halogenated Flame Retardant PC/ABS Alloy
Features:Halogen free flame retardant, V-0/1.5mmExcellent balance propertiesHigh heat resistanceGood chemical resistanceGood hydrolysis resistanceSuit for paint and electo-platingDrop down resistanc..
Back Pressure 0.000 - 0.700 MPa
0.000 - 102 psi
Kingfa JH-R2G10 P60 10% Glass Fiber Reinforced PC/ABS Alloy
Features:UL HB @ 1.6-3.2mmExcellent balance propertiesHigh stiffnessGood size stabilityGood surface adhesionExcellent processing properties, large partsApplications:Injection moldingAutomobile instr..
Back Pressure 0.300 - 0.700 MPa
43.5 - 102 psi
Kingfa LONOY 1200 PC/PBT Alloy
Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine..
Back Pressure 0.300 - 0.700 MPa
43.5 - 102 psi
Kingfa LONOY 1600 PC/PBT Alloy
Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine..
Back Pressure 0.300 - 0.700 MPa
43.5 - 102 psi
Kingfa LONOY 3010 Glass Fiber Reinforced PC/PBT Alloy
Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingElectric and electronic partsBusiness machine cabinetGarden to..
Back Pressure 0.300 - 0.700 MPa
43.5 - 102 psi
Kingfa LONOY 6100 Flame Retardant PC/PBT Alloy
Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingElectric and electronic partsBusiness machine cabinetGarden to..
Back Pressure 0.300 - 0.700 MPa
43.5 - 102 psi
Kingfa JH710 G30 Flame Retardant & 30% Glass Fiber Reinforced PC
Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc..
Back Pressure 0.300 - 0.700 MPa
43.5 - 102 psi
Kingfa LONOY 2100 LT PC/PET Alloy
Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine..
Back Pressure 0.300 - 0.700 MPa
43.5 - 102 psi
Kingfa LONOY 2200 HT PC/PET Alloy
Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine..
Back Pressure 0.300 - 0.700 MPa
43.5 - 102 psi
BLUESTAR PBT 6630 30% Glass Filled
PBT6630 is an injection molding grade, with 30% glass fiber reinforced, high heat stability, and electrical properties, easy to process. It is widely used in automotive, home appliance, E/E industry..