Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger TECASINT 4051 Polyimide, Beige, 30% Glass Fiber (PI)

Category Polymer , Thermoplastic , Polyimide, Thermoplastic , Thermoplastic Polyimide, Glass Fiber
Manufacturer Ensinger
Trade Name TECASINT
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger TECASINT 4051 Polyimide, Beige, 30% Glass Fiber (PI).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excellent wear resistance among other things. The TECASINT 2000 series offers these enhanced thermal properties along with lower moisture absorption, a higher degree of toughness, and better machining properties. TECASINT 2011 is unfilled, while TECASINT 2021 contains 15% graphite which offer improved wear resistance and a lower coefficient of friction. TECASINT 2000 series with their superior physical properties, are ideal for application in the aerospace, nuclear, automotive, electrical/electronics, and chemical processing industries.Main features: High thermal and mechanical capacity, very creep resistant, high gamma radiation resistance, very low water absorption, good chemical resistance, low coefficient of thermal expansion, easily machined to tight tolerances, very good electrical insulation, flame retardant according to UL94 V-0Applications: Mechanical engineering, electronics, cryogenics, nuclear and vacuum technology, aircraft and aerospace industries, semiconductor technology, electrical engineeringPreferred Fields: Valve seating, switch parts, insulators, lead backerInformation Provided by Ensinger Sintimid
Physical Properties Metric English Comments
Density 1.65 g/cc
0.0596 lb/in³
DIN 53 479
Water Absorption 0.060 %

@Temperature 23.0 °C
0.060 %

@Temperature 73.4 °F
24 hours in water; EN ISO 62
0.26 %

@Temperature 80.0 °C
0.26 %

@Temperature 176 °F
24 hours in water; EN ISO 62
Mechanical Properties Metric English Comments
Hardness, Shore D 90

@Temperature 23.0 °C
90

@Temperature 73.4 °F
DIN 53 505
Tensile Strength 77.0 MPa

@Temperature 23.0 °C
11200 psi

@Temperature 73.4 °F
EN ISO 527
Elongation at Break 1.2 %

@Temperature 23.0 °C
1.2 %

@Temperature 73.4 °F
EN ISO 527
Elongation at Yield 2.3 %

@Temperature 23.0 °C
2.3 %

@Temperature 73.4 °F
Flexural Elongation; EN ISO 178
Tensile Modulus 7.20 GPa

@Temperature 23.0 °C
1040 ksi

@Temperature 73.4 °F
EN ISO 527
Flexural Strength 136 MPa

@Temperature 23.0 °C
19700 psi

@Temperature 73.4 °F
EN ISO 178
Flexural Modulus 6.40 GPa

@Temperature 23.0 °C
928 ksi

@Temperature 73.4 °F
EN ISO 178
Compressive Yield Strength 193 MPa

@Strain 10.0 %,
Temperature 23.0 °C
28000 psi

@Strain 10.0 %,
Temperature 73.4 °F
EN ISO 604
Compressive Strength 259 MPa

@Temperature 23.0 °C
37600 psi

@Temperature 73.4 °F
EN ISO 604
Compressive Modulus 2.74 GPa

@Temperature 23.0 °C
397 ksi

@Temperature 73.4 °F
EN ISO 604
Charpy Impact Unnotched 1.97 J/cm²

@Temperature 23.0 °C
9.37 ft-lb/in²

@Temperature 73.4 °F
EN ISO 179
Charpy Impact, Notched 0.500 J/cm²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
EN ISO 179
Compression Set 42.8 %

@Temperature 23.0 °C
42.8 %

@Temperature 73.4 °F
Compression at Break; EN ISO 604
Thermal Properties Metric English Comments
CTE, linear 38.0 µm/m-°C

@Temperature 50.0 - 200 °C
21.1 µin/in-°F

@Temperature 122 - 392 °F
DIN 53 752
47.0 µm/m-°C

@Temperature 200 - 300 °C
26.1 µin/in-°F

@Temperature 392 - 572 °F
DIN 53 752
CTE, linear, Transverse to Flow 51.0 µm/m-°C

@Temperature 50.0 - 200 °C
28.3 µin/in-°F

@Temperature 122 - 392 °F
DIN 53 752
70.0 µm/m-°C

@Temperature 200 - 300 °C
38.9 µin/in-°F

@Temperature 392 - 572 °F
DIN 53 752
Thermal Conductivity 0.400 W/m-K

@Temperature 40.0 °C
2.78 BTU-in/hr-ft²-°F

@Temperature 104 °F
ISO 8302
Electrical Properties Metric English Comments
Volume Resistivity 1.80e+16 ohm-cm

@Temperature 23.0 °C
1.80e+16 ohm-cm

@Temperature 73.4 °F
IEC 60093
Surface Resistivity per Square 9.40e+16 ohm

@Temperature 23.0 °C
9.40e+16 ohm

@Temperature 73.4 °F
IEC 60093
Dielectric Constant 3.59

@Frequency 1000 Hz,
Temperature 23.0 °C
3.59

@Frequency 1000 Hz,
Temperature 73.4 °F
IEC 60250