Polymer Property : CTE, linear = 47.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 47.0 µm/m-°C

@Temperature 0.000 - 100 °C
26.1 µin/in-°F

@Temperature 32.0 - 212 °F
X-Direction; 5°C/min; ASTM D3386
Rogers Corporation RT/duroid® 6006 Ceramic-PTFE Composite Microwave Laminate
Features:High dielectric constant for circuit size reductionLow loss - Ideal for operating at X-band or belowTight dielectric constant and thickness control for repeatable circuit performanceLow moi..
CTE, linear 47.0 µm/m-°C

@Temperature 0.000 - 100 °C
26.1 µin/in-°F

@Temperature 32.0 - 212 °F
Z-Direction; 5°C/min; ASTM D3386
Rogers Corporation RT/duroid® 6010.2LM Ceramic-PTFE Composite Microwave Laminate
Features:High dielectric constant for circuit size reductionLow loss - Ideal for operating at X-band or belowLow Z-axis expansion. Provides reliable plated through holes in multi-layer boardsTight ..
CTE, linear 47.0 µm/m-°C

@Temperature <=100 °C
26.1 µin/in-°F

@Temperature <=212 °F
ISO E 830
Wolf Kunststoff ZEDEX® ZX-324V1T A3H PEEK Polymer, Reinforced
Main Characteristics: High resilience; High elasticity; Low permanent deformation; Stress resistant; High strength at temperatures above 140 ° CApplications: Shipbuilding; Chemical Engineering; Aut..
CTE, linear 47.0 µm/m-°C

@Temperature <=150 °C
26.1 µin/in-°F

@Temperature <=302 °F
ISO E 831
Wolf Kunststoff ZEDEX® ZX-750V5T A9T Polymer Alloy
Main Characteristics: Hard; Stiff; Tough; High dimensional stability; High fatigue strength; High weather resistance; Good fire behavior; Suitable for vacuum; Good machinability; Contains PTFE; Stre..
CTE, linear 47.0 µm/m-°C

@Temperature 10.0 - 50.0 °C
26.1 µin/in-°F

@Temperature 50.0 - 122 °F
Alpha 1
Tra-Con Tra-Bond 526M05 Rapid Low Temperature Cure Adhesive
TRA-BOND 526M05 is a low viscosity, fast cure at low temperature, long pot-life adhesive. Information provided by Tra-Con Inc.
CTE, linear 47.0 µm/m-°C

@Temperature 200 - 300 °C
26.1 µin/in-°F

@Temperature 392 - 572 °F
DIN 53 752
Ensinger TECASINT 4051 Polyimide, Beige, 30% Glass Fiber (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
CTE, linear 47.0 µm/m-°C

@Temperature 50.0 - 200 °C
26.1 µin/in-°F

@Temperature 122 - 392 °F
DIN 53 752
Ensinger TECASINT™ 2021 Polyimide, Brown (PI)
TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications...