Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 259 MPa | 37500 psi | |
SGL Carbon Group EK 3205 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Compressive Strength | 259 MPa @Temperature 23.0 °C |
37600 psi @Temperature 73.4 °F |
EN ISO 604 |
Ensinger TECASINT 4051 Polyimide, Beige, 30% Glass Fiber (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |