Thermal Properties Metric English Comments
CTE, linear 38.0 µm/m-°C

@Temperature -53.9 - 22.2 °C
21.1 µin/in-°F

@Temperature -65.0 - 72.0 °F
Malvern Minerals Epoxy with 50% Novacite® Daper Quartz Filler
Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo..
CTE, linear 38.0 µm/m-°C

@Temperature 22.2 - 73.9 °C
21.1 µin/in-°F

@Temperature 72.0 - 165 °F
Malvern Minerals Epoxy with 50% Novacite® Daper Quartz Filler
Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo..
CTE, linear 38.0 µm/m-°C

@Temperature -53.9 - 73.9 °C
21.1 µin/in-°F

@Temperature -65.0 - 165 °F
Malvern Minerals Epoxy with 50% Novacite® Daper Quartz Filler
Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo..
CTE, linear 38.0 µm/m-°C

@Temperature 100 - 200 °C
21.1 µin/in-°F

@Temperature 212 - 392 °F
ASTM E-233
UBE UPIMOL® S High Heat Polyimide Shape
Description: Ube's UPIMOL is an exceptionally heat-resistant polyimide Shape. This product has the same molecular structure as UPILEX, an ultra-high heat-resistant polyimide film developed by Ub..
CTE, linear 38.0 µm/m-°C

@Temperature <=150 °C
21.1 µin/in-°F

@Temperature <=302 °F
ISO E 831
Wolf Kunststoff ZEDEX® ZX-324VMT A3B PEEK, Fiber Reinforced
Main Characteristics: Maximum rigidity; Very good wear resistance; Low stick-slip tendency; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInfor..
CTE, linear 38.0 µm/m-°C

@Temperature <=100 °C
21.1 µin/in-°F

@Temperature <=212 °F
ISO E 830
Wolf Kunststoff ZEDEX® ZX-530CD3 031 Polymer Alloy, Fiber Reinforced and PTFE Modified
Main Characteristics: Dimensionally stable and rigid; Stress resistant; Extremely low wear to 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsIn..
CTE, linear 38.0 µm/m-°C

@Temperature <=100 °C
21.1 µin/in-°F

@Temperature <=212 °F
ISO E 830
Wolf Kunststoff ZEDEX® ZX-530EL3 066 Polymer Alloy, Carbon Fiber Reinforced
Main Characteristics: Low thermal expansion; High rigidity; High yield stress; High wear resistance; Low friction; Stress ResistantApplications: Chemical Engineering; Laboratory Technology; Automitv..
CTE, linear 38.0 µm/m-°C

@Temperature 50.0 - 200 °C
21.1 µin/in-°F

@Temperature 122 - 392 °F
DIN 53 752
Ensinger TECASINT 4051 Polyimide, Beige, 30% Glass Fiber (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
CTE, linear 38.0 µm/m-°C

@Temperature 200 - 300 °C
21.1 µin/in-°F

@Temperature 392 - 572 °F
DIN 53 752
Ensinger TECASINT™ 2031 Polyimide, 40% Graphite Filled (PI)
TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications...
CTE, linear 38.0 µm/m-°C

@Temperature 0.000 - 120 °C
21.1 µin/in-°F

@Temperature 32.0 - 248 °F
100 x 15 x 3 mm sample; AZDEL Test
Azdel Plus C200B01N 20% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C200B01 is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a v..
CTE, linear 38.0 µm/m-°C

@Temperature 0.000 - 120 °C
21.1 µin/in-°F

@Temperature 32.0 - 248 °F
100 x 15 x 3 mm sample; AZDEL Test
Azdel Plus C220B02N 22% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C220B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a ..