Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 38.0 µm/m-°C @Temperature -53.9 - 22.2 °C |
21.1 µin/in-°F @Temperature -65.0 - 72.0 °F |
|
Malvern Minerals Epoxy with 50% Novacite® Daper Quartz Filler Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo.. |
|||
CTE, linear | 38.0 µm/m-°C @Temperature 22.2 - 73.9 °C |
21.1 µin/in-°F @Temperature 72.0 - 165 °F |
|
Malvern Minerals Epoxy with 50% Novacite® Daper Quartz Filler Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo.. |
|||
CTE, linear | 38.0 µm/m-°C @Temperature -53.9 - 73.9 °C |
21.1 µin/in-°F @Temperature -65.0 - 165 °F |
|
Malvern Minerals Epoxy with 50% Novacite® Daper Quartz Filler Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo.. |
|||
CTE, linear | 38.0 µm/m-°C @Temperature 100 - 200 °C |
21.1 µin/in-°F @Temperature 212 - 392 °F |
ASTM E-233 |
UBE UPIMOL® S High Heat Polyimide Shape Description: Ube's UPIMOL is an exceptionally heat-resistant polyimide Shape. This product has the same molecular structure as UPILEX, an ultra-high heat-resistant polyimide film developed by Ub.. |
|||
CTE, linear | 38.0 µm/m-°C @Temperature <=150 °C |
21.1 µin/in-°F @Temperature <=302 °F |
ISO E 831 |
Wolf Kunststoff ZEDEX® ZX-324VMT A3B PEEK, Fiber Reinforced Main Characteristics: Maximum rigidity; Very good wear resistance; Low stick-slip tendency; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInfor.. |
|||
CTE, linear | 38.0 µm/m-°C @Temperature <=100 °C |
21.1 µin/in-°F @Temperature <=212 °F |
ISO E 830 |
Wolf Kunststoff ZEDEX® ZX-530CD3 031 Polymer Alloy, Fiber Reinforced and PTFE Modified Main Characteristics: Dimensionally stable and rigid; Stress resistant; Extremely low wear to 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsIn.. |
|||
CTE, linear | 38.0 µm/m-°C @Temperature <=100 °C |
21.1 µin/in-°F @Temperature <=212 °F |
ISO E 830 |
Wolf Kunststoff ZEDEX® ZX-530EL3 066 Polymer Alloy, Carbon Fiber Reinforced Main Characteristics: Low thermal expansion; High rigidity; High yield stress; High wear resistance; Low friction; Stress ResistantApplications: Chemical Engineering; Laboratory Technology; Automitv.. |
|||
CTE, linear | 38.0 µm/m-°C @Temperature 50.0 - 200 °C |
21.1 µin/in-°F @Temperature 122 - 392 °F |
DIN 53 752 |
Ensinger TECASINT 4051 Polyimide, Beige, 30% Glass Fiber (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
CTE, linear | 38.0 µm/m-°C @Temperature 200 - 300 °C |
21.1 µin/in-°F @Temperature 392 - 572 °F |
DIN 53 752 |
Ensinger TECASINT™ 2031 Polyimide, 40% Graphite Filled (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |
|||
CTE, linear | 38.0 µm/m-°C @Temperature 0.000 - 120 °C |
21.1 µin/in-°F @Temperature 32.0 - 248 °F |
100 x 15 x 3 mm sample; AZDEL Test |
Azdel Plus C200B01N 20% Chopped Fiber Mat / PP Resin Matrix AZDEL® C200B01 is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a v.. |
|||
CTE, linear | 38.0 µm/m-°C @Temperature 0.000 - 120 °C |
21.1 µin/in-°F @Temperature 32.0 - 248 °F |
100 x 15 x 3 mm sample; AZDEL Test |
Azdel Plus C220B02N 22% Chopped Fiber Mat / PP Resin Matrix AZDEL® C220B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |