Electrical Properties Metric English Comments
Volume Resistivity 1.80e+16 ohm-cm
1.80e+16 ohm-cm
150°C for 1,000 hrs
Fujipoly Industries Sarcon® 15GHR Thin-Film GHR
Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of ..
Volume Resistivity 1.80e+16 ohm-cm
1.80e+16 ohm-cm
200°C for 1,000 hrs
Fujipoly Industries Sarcon® 15GHR Thin-Film GHR
Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of ..
Volume Resistivity 1.80e+16 ohm-cm
1.80e+16 ohm-cm
200°C for 1,000 hrs
Fujipoly Industries Sarcon® 20GHR Thin-Film GHR
Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of ..
Volume Resistivity 1.80e+16 ohm-cm
1.80e+16 ohm-cm
ASTM D257
SABIC Innovative Plastics Valox® 865 PBT+PET
30% GR PBTP, UL94 V-0 rated. Non-blooming flame retardant. Improved surface appearance. Same application areas as for VALOX 855.
Volume Resistivity 1.80e+16 ohm-cm
1.80e+16 ohm-cm
ASTM D257
SABIC Innovative Plastics Valox® 865 PBT+PET (Asia Pacific)
30% GR PBTP, UL94 V-0 rated. Non-blooming flame retardant. Improved surface appearance. Same application areas as for VALOX 855.
Volume Resistivity 1.80e+16 ohm-cm
1.80e+16 ohm-cm
ASTM D257
SABIC Innovative Plastics NORYL N190X PPE+HIPS (Asia Pacific)
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. Dielectric strength. Suitable for E/E market applications.
Volume Resistivity 1.80e+16 ohm-cm
1.80e+16 ohm-cm
ASTM D257
SABIC Innovative Plastics NORYL N190X PPE+PS
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. RTI Elec/Imp/Str 95/80/95. Dielectric strength. Suitable for E/E market applications.
Volume Resistivity 1.80e+16 ohm-cm
1.80e+16 ohm-cm
GB/T1410-2006
Sichuan Deyang Haton® hMR60DL Polyphenylene Sulfide, Glass & Mineral Reinforced
Injection molding, low chlorineInformation provided by Sichuan Deyang Chemical Co., LTD
Volume Resistivity 1.80e+16 ohm-cm
1.80e+16 ohm-cm
ASTM D-257
UBE UPIMOL® R Polyimide Shape
Description: Ube's UPIMOL is an exceptionally heat-resistant polyimide Shape. This product has the same molecular structure as UPILEX, an ultra-high heat-resistant polyimide film developed by Ub..
Volume Resistivity 1.80e+16 ohm-cm

@Temperature 23.0 °C
1.80e+16 ohm-cm

@Temperature 73.4 °F
IEC 60093
Ensinger TECASINT 4051 Polyimide, Beige, 30% Glass Fiber (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..