Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 2.74 GPa @Temperature 23.0 °C |
397 ksi @Temperature 73.4 °F |
EN ISO 604 |
Ensinger TECASINT 4051 Polyimide, Beige, 30% Glass Fiber (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Compressive Modulus | 2.74 GPa | 397 ksi | ASTM D695 |
DuPont Teijin Films Mylar® A Polyester Film, 1400 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |