Polymer Property : Surface Resistivity per Square = 9.40e+16 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistivity per Square 9.40e+16 ohm

@Temperature 23.0 °C
9.40e+16 ohm

@Temperature 73.4 °F
IEC 60093
Ensinger TECASINT 4051 Polyimide, Beige, 30% Glass Fiber (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..