Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 77.2 MPa | 11200 psi | ASTM D638 |
Techmer ES Elastoblend® TPX-PA6/6 97058 BK 32% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Fiber Reinforcement, 33% Filler by WeightAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedUL File.. |
|||
Tensile Strength | 77.2 MPa | 11200 psi | ASTM D638 |
Solvay Specialty Polymers Acudel® 22000 Polyphenylsulfone, Modified (PPSU, Modified) Acudel® 22000 is a modified polyphenylsulfone. It is a high-heat, high-performance resin formulation exhibiting very good hydrolytic stability, excellent resistance to acids and bases and good re.. |
|||
Tensile Strength | 77.2 MPa | 11200 psi | ASTM D638 |
Techmer ES Elastoblend® PA6/6 IM 3757 HS L Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Fast Molding Cycle, High Flow, Heat Stabilized, Lubricant and Impact ModifiedProcessing Met.. |
|||
Tensile Strength | 77.0 MPa @Temperature 23.0 °C |
11200 psi @Temperature 73.4 °F |
EN ISO 527 |
Ensinger TECASINT 4051 Polyimide, Beige, 30% Glass Fiber (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Tensile Strength | 77.0 MPa @Temperature 23.0 °C |
11200 psi @Temperature 73.4 °F |
EN ISO 527 |
Ensinger TECASINT™ 2022 Polyimide, Black, 15% Graphite (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |
|||
Tensile Strength | 77.2 MPa | 11200 psi | ASTM D638 |
Ensinger Tecatron® XP-86 Compression Molded PPS Compound, with 40% Carbon Fiber Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Tensile Strength | 77.2 MPa | 11200 psi | Cross; ASTM D882 |
Arlon DiClad 870 PTFE/Woven Fiberglass Laminate Extremely Low Loss TangentExcellent Dimensional StabilityProduct Performance UniformityBenefits:Electrical Properties are highly uniform across frequencyConsistent Mechanical PerformanceExcellent Ch.. |
|||
Tensile Strength | 77.0 MPa | 11200 psi | ISO 527 |
Lucite International Diakon® ST15G8 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed by in.. |