Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Engineered Polymer Solutions PBT VM 450, 20% Mineral Filled

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Mineral Filled
Manufacturer Engineered Polymer Solutions
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Engineered Polymer Solutions PBT VM 450, 20% Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Plate-able. Natural and colors available. Injection molding grade. Uses: Automotive, appliancesInformation provided by Engineered Polymer Solutions.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ASTM D792-91
Viscosity Measurement 1500

@Temperature 250 °C
1500

@Temperature 482 °F
in-sec Melt Viscosity; 5.0 kg; ASTM D1238 Mod.
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 57.9 MPa
8400 psi
ASTM D638
Flexural Modulus 4.14 GPa
600 ksi
ASTM D790
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 188 °C
370 °F
1/4 inch bar; ASTM D648
Processing Properties Metric English Comments
Rear Barrel Temperature 238 - 254 °C
460 - 490 °F
Middle Barrel Temperature 243 - 260 °C
470 - 500 °F
Front Barrel Temperature 249 - 266 °C
480 - 510 °F
Nozzle Temperature 243 - 260 °C
470 - 500 °F
Melt Temperature 249 - 266 °C
480 - 510 °F
Mold Temperature 71.1 - 93.3 °C
160 - 200 °F
Drying Temperature 121 °C
250 °F
Dry Time 3 - 4 hour
3 - 4 hour
Moisture Content 0.20 %
0.20 %
Back Pressure 0.345 - 0.689 MPa
50.0 - 100 psi
Users viewing this material also viewed the following: