Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
Oxford Polymers Oxnilon 66-13GF 13% Glass Fiber Filled Nylon 66 for Injection Molding 13% Glass Fiber Filled Nylon 66 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DFL22 PC (Asia Pacific) LNP* Lubricomp* DFL22 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
Technetics Group Amicon™ PEEK
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6 GF15 IM L 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GB30 FR 30% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 30% Filler by WeightAdditive: LubricantFeatures: Flame Retardant and LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
Techmer ES HiFill® HDPE GF30 CC 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GB20 L BK 20% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 20% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GB30 L 30% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF/M20 IM BK 20% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by Weight and Mineral Filler, 20% Filler by WeightAdditive: Lubricant, Impact Modifier and Heat S.. |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
Techmer ES Statiblend® ABS GF15 AS 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightAdditive: AntistaticFeatures: AntistaticInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
Entec Hylex® P1025G10NHFR Polycarbonate, 10% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Flexural Modulus | 4.14 - 15.5 GPa | 600 - 2250 ksi | Average value: 9.47 GPa Grade Count:34 |
Overview of materials for Nylon 66, Glass Fiber/MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/MoS2 Filled". Each property range of values reported is minimum and maximum values.. |
|||
Flexural Modulus | 4.14 GPa | 600 ksi | ASTM D790 |
PolyOne Edgetek® PE-30GF/000 WHITE High Density Polyethylene (HDPE), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedWhitePolyOne First ChoiceInformation provided by PolyOne Corporation. |