Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
Nilit FRIANYL B63 KF50 Nylon 6 for injection molding, 50% short glass fiber reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Density 1.50 - 1.55 g/cc
0.0542 - 0.0560 lb/in³
Average value: 1.52 g/cc Grade Count:4
Overview of materials for PVC, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PVC, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are included. E..
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
Hexion Bakelite™ PF 12404 Phenolic Formaldehyde Resin, High Surface Quality, Low Shrinkage  (discontinued **)&
Phenolic molding compound, inorganically/organically filled, good dimensional stability, low shrinkage.Application areas: Housing parts for gas meter.Information provided by Bakelite AGBakelite AG b..
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
Menzolit Menzolit® SMC 0500 Unsaturated Polyester UP
SMC 0500 is a special SMC with reduced density. The glass level has been selected to combine good moulding with good strength and stiffness properties. Even without a specific fire retardant the fir..
Density 1.50 - 1.55 g/cc
0.0542 - 0.0560 lb/in³
320 Resin
Lord Adhesives 320 / 322 Epoxy Adhesive
LORD® 320/322 adhesive is a general purpose, two component epoxy adhesive system formulated for primerless adhesion to automotive sheet molded compounds (SMC). This adhesive system also provides ..
Density 1.50 g/cc
0.0542 lb/in³
ISO R 1183
Multibase Multibatch® MP 52659 Sheet Extrusion
HPP. 60% Talc Filled.Lamellar talcInformation provided by Multibase
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
SABIC Innovative Plastics LNP Lubricomp JX91055 PES (Europe-Africa-Middle East)
LNP* LUBRICOMP* JX91055 is a compound based on Polyethersulfone resin containing Carbon Fiber and Proprietary Lubricant . Added features include Internally Lubricated and Electrically Conductive.Thi..
Density 1.50 g/cc
0.0542 lb/in³
ASTM D792
Techmer ES Luriblend® PA6/6 GF33 TL15 BK 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Heat Stab..
Density 1.50 g/cc
0.0542 lb/in³
ASTM D792
Chase Plastics CP Pryme® N340HL (Dry) Nylon 6, 40% Glass Fiber Reinforced, Heat Stabilized, Lubricated, Recycled Content
Features: Heat stabilizedLubricatedRecycled contentForm: PelletsInformation provided by Chase Plastics.
Density 1.50 g/cc
0.0542 lb/in³
Von Roll Isola IMI Transtherm® TP 1000-9 Polyester, Fiberglass Reinforced, Boron Nitride Filled, for Thermal Management
Data provided by Von Roll Isola USA.Transtherm thermal management products are used as an interface between a heat generating device and the heat sink to minimize thermal resistance and to provide e..
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183-87
Wellman EcoLon® MRGF1914-BK1 Nylon 66, 40% Mineral and Glass Reinforced
All information provided by Wellman Engineered Resins.
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183-87
Wellman Wellamid® GF43-66/6 XE-NBK1 43% Glass Fiber Reinforced, Engineering Grade Nylon 66/6
Description: Glass Fiber Reinforced, Engineering Grade Nylon 66/6Information provided by Wellman.
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183-87
Wellman Wellamid® MRGF25/15 42H-NBK1 40% Mineral/Glass Fiber Reinforced Nylon 6
Description: Mineral/Glass Fiber Reinforced Nylon 6Information provided by Wellman.
Density 1.50 g/cc
0.0542 lb/in³
DIN 53479
Polyram RamTough PZ300G8 Polycarbonate, 40% Glass Fiber
40% Glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind.
Density 1.50 g/cc
0.0542 lb/in³
Cured
Chesterton ARC S1 General purpose coating
Description: An advanced polymer composite formulated to protect metal surfaces from corrosion and chmical attack. It is normally applied at a thickness of 250 microns (10 mils) per coat. Non-shrink..
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
DSM Akulon® K224-TG9 Nylon 6-45% Glass Reinforced (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
DuPont Performance Polymers Crastin® LW9020FR BK851 PBT+ASA  (Unverified Data**)
20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020FR BK851 is a 20% glass fiber reinforced flame retardant black polybutylene tere..
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
Eurostar Starflam P10003 PA6, Mineral Filled, Flame Retardant, Extrusion
Starflam P10003 is a Mineral Filled, Halogen Free, Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Density 1.50 - 1.54 g/cc
0.0542 - 0.0556 lb/in³
IEC 60811
Fainplast Compounds HAX HF 045 Halogen Free PVC
General purpose; improved fire performance
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
Eurotec® Tecomid® NBX0 HF75 NL PA6, 75% heavy reinforced, improved flexibility, natural
Information provided by Eurotec®
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
Celanese CELANEX 3309HRT PBT, 30% Glass Reinforced
Celanex 3309HRT is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate that has excellent hydrolysis resistance, toughness and improved flow.Information provided by Celanese
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
Celanese VECTRA A230 LCP, 30% Specialty
Exceptional stiffness. Electrically conductive. 30% carbon fiber reinforced.Information provided by Celanese
Density 1.50 g/cc
0.0542 lb/in³
ASTM D792 Method A
Arlon 45NK Woven Kevlar® Reinforced Laminate and Prepreg
45NK is a woven Kevlar® aramid fiber reinforced multifunctional epoxy laminate system engineered to provide in-plane CTE values as low as 6 ppm/°C for compatibility with leadless alumina ceramic c..
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
Akro-Plastic Akromid® T6 GF30 (3501) PPA Conditioned, 30% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
Density 1.50 g/cc
0.0542 lb/in³
ASTM D792
Beijing Chemical Industry KAIFA® 301-G20F PBT Resin
20% glass fiber reinforced, flame retardant, good flow, low bleedingInformation provided by Beijing Chemical Industry Research Institute (Group)
Density 1.50 g/cc
0.0541 lb/in³
Unifrax Fiberfrax® QF-180™ Blue Coating Cement
Fiberfrax QF-180™, QF-180™ Blue, and QF-150™ coating cements provide a range of consistencies for brush, spray, and trowel-on application. These coatings have 1260°C (2300°F) temperature grade..
Density 1.50 g/cc
0.0542 lb/in³
BASF Sico® Fast Red L 3855 Color Additive
Description: Naphthol-AS-red pigment with good fastness properties in full shadeChemical Structure: Naphthol-AS-redSuitable for: Waterborn systems, Acrylic-isocyanate systems, Acid curing system, Am..
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
SABIC Innovative Plastics Valox® VX4510 PBT (Europe-Africa-Middle East)
VALOX VX4510 is a flame retarded, 10% glassfiber reinforced injection moulding PBT resin.
Density 1.50 g/cc
0.0542 lb/in³
DIN 53479
Polyram RamOfin PPC371B50 Polypropylene, 50% Mineral Filled
50% mineral filled, heavy density polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind.
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
BASF Ultramid® 1603-2 NF2004 43% Glass Filled PA66 (Dry)
Ultramid 1603-2 NF2004 is a 43% glass reinforced, heat stabilized injection molding nylon 6/6 with the highest level of glass reinforcement for maximum strength and stiffness.