Polymer Property : Tensile Strength, Yield = 8400 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 57.9 MPa
8400 psi
Type I, 51 mm/min; ASTM D638
PolyOne Trilliant™ HC HC5220-0040 RS Natural Polypropylene, Unspecified (PP, Unspecified)
The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead..
Tensile Strength, Yield 57.9 MPa
8400 psi
ASTM D638
Polymer Resources PC/ABS-FR1 Flame Retardant PC/ABS Alloy
PC/ABS Alloy, Flame Retardant, Standard FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided..
Tensile Strength, Yield 57.9 MPa
8400 psi
ASTM D638
Polymer Resources PC/ABS-FR1-[color]-WR Flame Retardant PC/ABS Alloy, Wear Resistant
PC/ABS Alloy, Flame Retardant, Standard Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info..
Tensile Strength, Yield 57.9 MPa
8400 psi
ASTM D638
Polymer Resources PC/ABS-FR2 Flame Retardant PC/ABS Alloy, High Flow
PC/ABS Alloy, Flame Retardant, Higher FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b..
Tensile Strength, Yield 57.9 MPa
8400 psi
ASTM D638
Polymer Resources PC/ABS-GP1-[color]-UV General Purpose PC/ABS Alloy, UV-stabilized
PC/ABS Alloy, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide..
Tensile Strength, Yield 57.9 MPa
8400 psi
ASTM D638
Polymer Resources PPX/NY GP1 PPO/Nylon 66 Alloy
Polyphenylene Oxide/Nylon 66 Alloy , General PurposeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
Tensile Strength, Yield 57.9 MPa
8400 psi
ASTM D638
Polymer Resources PPX/NY GP2 PPO/Nylon 66 Alloy, Medium Heat
Polyphenylene Oxide/Nylon 66 Alloy , General Purpose, Medium HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
Tensile Strength, Yield 57.9 MPa
8400 psi
ASTM D638
Polymer Resources PC/ABS-FR1-[color]-UV Flame Retardant PC/ABS Alloy, UV-stabilized
PC/ABS Alloy, Flame Retardant, Standard Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
Tensile Strength, Yield 57.9 MPa
8400 psi
ASTM D638
Polymer Resources PC/ABS-GP1 General Purpose PC/ABS Alloy
PC/ABS Alloy, General Purpose Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Re..
Tensile Strength, Yield 57.9 MPa
8400 psi
ASTM D638
Polymer Resources PC/ABS-GP1-[color]-EP General Purpose PC/ABS Alloy, Electroplating Grade
PC/ABS Alloy, General Purpose, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p..
Tensile Strength, Yield 57.9 MPa
8400 psi
ASTM D638
Polymer Resources PC/ABS-GP1-[color]-LG General Purpose PC/ABS Alloy, Low Gloss Grade
PC/ABS Alloy, General Purpose, Low Gloss GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provid..
Tensile Strength, Yield 57.9 MPa
8400 psi
ASTM Data
Dow Isoplast® 151 Polyurethane (PUR-RT), Impact Modified  (discontinued **)
ISOPLAST® 151 resin is an impact modified amorphous polymer with the chemical resistance of crystalline resins. Its outstanding properties include excellent chemical resistance, high heat, low mois..
Tensile Strength, Yield 57.9 MPa
8400 psi
ASTM D638
Ravago Manufacturing Americas Hylon® N1000STHL HF Nylon 6/6  (discontinued **)
Available in North America Additive: Heat Stabilizer and LubricantFeatures: Lubricated, Heat Stabilized, High Flow and Ultra High ToughnessRoHS CompliantAuto Specifications: DELPHI DCM 4849 Color: B..
Tensile Strength, Yield 57.9 MPa

@Thickness 3.17 mm,
Temperature 22.8 °C
8400 psi

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D638
MRC Polymers NAXELLâ„¢ PC210MR General Purpose Polycarbonate, Medium MFR, with Release
Medium melt without impact modificationMFR can be modified between 10 to 40 g/10minCan be UV stabilizedInternal and external lubricant can be addedGenerally for black and gray colors onlyFR package ..
Tensile Strength, Yield 57.9 MPa
8400 psi
ASTM D638
Techmer ES HiFill® PA6 0301
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High DensityProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Tensile Strength, Yield 57.9 MPa
8400 psi
ASTM D638
Techmer ES Luriblend® POM CO TL15 Acetal
Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Low Friction and CopolymerInformation provided by TP Composites, Inc.
Tensile Strength, Yield 57.9 MPa
8400 psi
ASTM D638
Techmer ES Plastiblend® PC/ABS 1000
Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc.
Tensile Strength, Yield 57.9 MPa
8400 psi
ASTM D638
Techmer ES Plastiblend® PC/ABS 1950
Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc.
Tensile Strength, Yield 57.9 MPa
8400 psi
ASTM D638
Styron CALIBREâ„¢ IM 401-18 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Tensile Strength, Yield 57.9 MPa
8400 psi
ASTM Data
Styron CALIBREâ„¢ IM 401 18 Polycarbonate, Impact Modified
CALIBRE® IM401 series resins are impact modified, UL listed polycarbonate resins which contain mold release. CALIBRE IM 401 polycarbonate resins exhibit an excellent balance of impact strength an..
Tensile Strength, Yield 57.9 MPa
8400 psi
50 mm/min; ASTM D638
Styron CALIBREâ„¢ IM 401-18 Polycarbonate Resin
Overview: CALIBREâ„¢ IM 401-18 Impact Modified Polycarbonate resin is available in opaque formulations that offer benefits ranging from superior low temperature impact strength to easy process wi..
Tensile Strength, Yield 57.9 MPa
8400 psi
0.125 in, injection molded, unannealed; ASTM D638
Styron EMERGEâ„¢ 4410-18 MFR Polycarbonate
EMERGEâ„¢ PC 4410-18 advanced resin is a high impact polycarbonate resin designed for Information Technology Equipment and Injection Molding Applications.Information provided by DowThis product l..
Tensile Strength, Yield 57.9 MPa

@Temperature 23.0 °C
8400 psi

@Temperature 73.4 °F
Hexcel® HexPly® F652 Bismaleimide Resin, Carbon Fabric Form
Material Description: F3G584-60; Fiber: T300-3K; T300/13.5 mils (0.343 mm) per plyInformation provided by HexCel
Tensile Strength, Yield 57.9 MPa
8400 psi
chs 2 in/min; ASTM D638
Diamond Polymers ABS 3501 GF-10
Description: Reinforced Grade, 10%Glass FilledInformation provided by Diamond Polymers, Inc.
Tensile Strength, Yield 57.9 MPa
8400 psi
ASTM D638
Engineered Polymer Solutions PBT VM 450, 20% Mineral Filled
Plate-able. Natural and colors available. Injection molding grade. Uses: Automotive, appliancesInformation provided by Engineered Polymer Solutions.
Tensile Strength, Yield 57.9 MPa

@Temperature 149 °C
8400 psi

@Temperature 300 °F
ASTM D638
Mitsui AURUM® PL450C Polyimide  (discontinued **)
AURUM PL450C is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, unfilled AURU..
Tensile Strength, Yield 57.9 MPa
8400 psi
ASTM D638
Polymer Resources PPX/NY GP1 Modified PPO, General Purpose PPX/Nylon 6,6 Alloy  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Tensile Strength, Yield 57.9 MPa
8400 psi
ASTM D638
Polymer Resources PPX/NY GP2 Modified PPO, Medium Heat PPX/Nylon 6,6 Alloy  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.