Ecomass® 705ZD70 Tungsten Filled ABS

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer Ecomass Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ecomass® 705ZD70 Tungsten Filled ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nontoxic Alternative to Lead (Pb) for radiation shielding applicationsHigh specific GravityTungsten Filled ABS compoundRigidGood ToughnessInformation provided by Technical Polymers
Physical Properties Metric English Comments
Specific Gravity 3.00 g/cc
3.00 g/cc
ISO 1183
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
Internal
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.0 MPa
4350 psi
ISO 527
Flexural Modulus 2.90 GPa
421 ksi
ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
ISO 180-A
Processing Properties Metric English Comments
Melt Temperature 249 - 288 °C
480 - 550 °F
Mold Temperature 37.8 - 65.6 °C
100 - 150 °F
Drying Temperature 71.1 - 82.2 °C
160 - 180 °F
Dry Time 2 - 4 hour
2 - 4 hour